PP AW161 TPC SINGAPORE
COSMOPLENE®
container、Household goods
High rigidity、Middle flow
UL
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
Impact resistance | Test Condition | Test Method | TPC SINGAPORE/AW161 |
---|---|---|---|
Impact strength of cantilever beam gap | 23°C | ASTM D256 | 75 J/m |
-20°C | ASTM D256 | 38 J/m |
hardness | Test Condition | Test Method | TPC SINGAPORE/AW161 |
---|---|---|---|
Rockwell hardness | R级 | ASTM D785 | 90 |
Mechanical properties | Test Condition | Test Method | TPC SINGAPORE/AW161 |
---|---|---|---|
elongation | 断裂 | ASTM D638 | 400 % |
tensile strength | 断裂 | ASTM D638 | 23.5 Mpa |
屈服 | ASTM D638 | 28.5 Mpa | |
Flexural modulus | ASTM D790 | 1170 Mpa |
flammability | Test Condition | Test Method | TPC SINGAPORE/AW161 |
---|---|---|---|
UL flame retardant rating | UL 94 | HB |
physical property | Test Condition | Test Method | TPC SINGAPORE/AW161 |
---|---|---|---|
Shrinkage rate | TD:2.00mm | 内部方法 | 1.5 % |
density | ASTM D792 | 0.900 g/cm³ | |
melt mass-flow rate | ASTM D1238 | 9.0 g/10min | |
Shrinkage rate | MD:2.00mm | 内部方法 | 1.5 % |
Thermal performance | Test Condition | Test Method | TPC SINGAPORE/AW161 |
---|---|---|---|
Heat distortion temperature | 0.45MPa,未退火,HDT | ASTM D648 | 117 °C |