PES SUMIPLOY® AS1411 SumiDurez Singapore Pte Ltd
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--

Plastic Datasheets

Impact resistanceTest ConditionTest MethodSumiDurez Singapore Pte Ltd/SUMIPLOY® AS1411
Impact strength of cantilever beam gap6.40mmASTM D25630 J/m
Suspended wall beam without notch impact strength6.40mmASTM D256220 J/m
hardnessTest ConditionTest MethodSumiDurez Singapore Pte Ltd/SUMIPLOY® AS1411
Rockwell hardnessR级ASTM D785125
Mechanical propertiesTest ConditionTest MethodSumiDurez Singapore Pte Ltd/SUMIPLOY® AS1411
elongation断裂ASTM D6383.7 %
tensile strength ASTM D63874.0 MPa
Flexural modulusASTM D7905400 MPa
bending strengthASTM D790105 MPa
flammabilityTest ConditionTest MethodSumiDurez Singapore Pte Ltd/SUMIPLOY® AS1411
UL flame retardant rating0.53mmUL 94V-0
physical property Test ConditionTest MethodSumiDurez Singapore Pte Ltd/SUMIPLOY® AS1411
Shrinkage rateMDASTM D9550.26 %
Water absorption rate24hrASTM D5700.50 %
densityASTM D7921.52 g/cm³
Shrinkage rateTDASTM D9550.36 %
Thermal performanceTest ConditionTest MethodSumiDurez Singapore Pte Ltd/SUMIPLOY® AS1411
Heat distortion temperature1.8MPa,未退火,HDTASTM D648209 °C
Linear coefficient of thermal expansionTD:50到150°CASTM D6964.6E-05 cm/cm/°C
MD:-50到150°CASTM D6962.9E-05 cm/cm/°C