Material Comparison
Product Info
Product Name
Brand Name
Usages
Properties
Certificates

TPEE ECO L460 DSM HOLAND
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
| hardness | Test Condition | Test Method | DSM HOLAND/ECO L460 |
|---|---|---|---|
| Shore hardness | Shore D, 3 Sec | ISO 868 | 45 |
| thermal performance | Test Condition | Test Method | DSM HOLAND/ECO L460 |
|---|---|---|---|
| Melting temperature | ISO 11357-3 | 180 °C | |
| Vicat softening temperature | ISO 306/B50 | 38.0 °C |
| mechanical properties | Test Condition | Test Method | DSM HOLAND/ECO L460 |
|---|---|---|---|
| Tensile modulus | ISO 527-2 | 85.0 Mpa | |
| tensile strength | 100% Strain | ISO 527-2 | 10.8 Mpa |
| 5.0% Strain | ISO 527-2 | 4.80 Mpa | |
| 50% Strain | ISO 527-2 | 10.8 Mpa | |
| Break | ISO 527-2 | 15.0 Mpa | |
| 10% Strain | ISO 527-2 | 7.70 Mpa |
| Electrical performance | Test Condition | Test Method | DSM HOLAND/ECO L460 |
|---|---|---|---|
| Dielectric strength | IEC 60243-1 | 20 KV/mm | |
| Volume resistivity | IEC 60093 | > 1.0E+15 ohms·cm |
| Physical properties | Test Condition | Test Method | DSM HOLAND/ECO L460 |
|---|---|---|---|
| Biobased content | CSA LISTED | 43 % | |
| Melt Volume Flow Rate (MVR) | 230°C/2.16 kg | ISO 1133 | 39.0 cm3/10min |
| Water absorption rate | Equilibrium, 23°C, 50% RH | ISO 62 | 0.030 % |
| flammability | Test Condition | Test Method | DSM HOLAND/ECO L460 |
|---|---|---|---|
| Flammability level | UL 94 | HB |