Material Comparison

Product Info
Product Name
Brand Name
Usages
Properties
Certificates
IR SIBUR Synthetic Rubber IR SKI-3 Group II SIBUR RUSSIA
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--

Plastic Datasheets

physical property Test ConditionTest MethodSIBUR RUSSIA/SIBUR Synthetic Rubber IR SKI-3 Group II
Stearic Acid内部方法0.60to1.4 %
Volatile compoundsASTM D5668<1.0 %
Mooney viscosityML1+4,100°CASTM D164667to76 MU
ash contentASTM D5667<0.60 %
elastomerTest ConditionTest MethodSIBUR RUSSIA/SIBUR Synthetic Rubber IR SKI-3 Group II
tensile strength 300%应变ASTM D3403>7.00 MPa
屈服ASTM D3403>27.0 MPa
elongation断裂ASTM D3403>500 %