| thermal performance | Test Condition | Test Method | DSM HOLAND/TE373 |
|---|---|---|---|
| Linear coefficient of thermal expansion | Across Flow | ISO 11359-2 | 1.1E-4 cm/cm/°C |
| Hot deformation temperature | 1.8 MPa, Unannealed | ISO 75-2/A | 190 °C |
| Linear coefficient of thermal expansion | Flow | ISO 11359-2 | 8.5E-5 cm/cm/°C |
| Melting temperature | ISO 11357-3 | 295 °C | |
| impact performance | Test Condition | Test Method | DSM HOLAND/TE373 |
| Charpy Notched Impact Strength | 23°C | ISO 179/1eA | 5.0 kJ/m² |
| -30°C | ISO 179/1eA | 4.0 kJ/m² | |
| Impact strength of cantilever beam gap | 23°C | ISO 180/1A | 5.0 kJ/m² |
| -40°C | ISO 180/1A | 4.0 kJ/m² | |
| Impact strength of simply supported beam without notch | 23°C | ISO 179/1eU | 150 kJ/m² |
| -30°C | ISO 179/1eU | 110 kJ/m² | |
| Physical properties | Test Condition | Test Method | DSM HOLAND/TE373 |
| density | ISO 1183 | 1.17 g/cm³ | |
| Water absorption rate | Equilibrium, 23°C, 50% RH | ISO 62 | 3.4 % |
| Shrinkage rate | Flow | ISO 294-4 | 2.0 % |
| 横向Flow | ISO 294-4 | 2.0 % | |
| mechanical properties | Test Condition | Test Method | DSM HOLAND/TE373 |
| Nominal tensile fracture strain | ISO 527-2 | 10 % | |
| tensile strength | Yield | ISO 527-2 | 85.0 Mpa |
| Bending modulus | ISO 178 | 2400 Mpa | |
| Tensile modulus | ISO 527-2 | 2800 Mpa |