Material Comparison
Product Info
Product Name
Brand Name
Usages
Properties
Certificates

PA6 Staramide BG8 EUROSTAR FRANCE
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
Impact resistance | Test Condition | Test Method | EUROSTAR FRANCE/Staramide BG8 |
---|---|---|---|
Impact strength of cantilever beam gap | -20°C | ISO 180/1A | 16 kJ/m² |
Impact strength of simply supported beam without notch | 23°C | ISO 179/1eU | 150 kJ/m² |
Impact strength of cantilever beam gap | 23°C | ISO 180/1A | 17 kJ/m² |
-40°C | ISO 180/1A | 15 kJ/m² |
Electrical performance | Test Condition | Test Method | EUROSTAR FRANCE/Staramide BG8 |
---|---|---|---|
relative permittivity | 60Hz | IEC 60250 | 3.60 |
50Hz | IEC 60250 | 3.60 | |
dielectric strength | 3.20mm,在油中 | IEC 60243-1 | 20 kV/mm |
Volume resistivity | IEC 60093 | >1.0E+16 ohms·cm | |
relative permittivity | 1MHz | IEC 60250 | 3.40 |
Surface Resistivity | IEC 60093 | >1.0E+16 ohms | |
Compared to the Leakage Tracking Index (CTI) | 解决方案B | IEC 60112 | PLC 2 |
-- | IEC 60112 | PLC 1 | |
Dissipation Factor | 50Hz | IEC 60250 | 6.1E-03 |
60Hz | IEC 60250 | 6.1E-03 | |
1MHz | IEC 60250 | 0.016 |
Mechanical properties | Test Condition | Test Method | EUROSTAR FRANCE/Staramide BG8 |
---|---|---|---|
tensile strength | 断裂 | ISO 527-2/5 | 195 MPa |
Tensile strain | 断裂 | ISO 527-2/5 | 2.0 % |
Flexural modulus | ISO 178 | 12000 MPa | |
Tensile modulus | ISO 527-2/1 | 13500 MPa | |
bending strength | ISO 178 | 290 MPa |
flammability | Test Condition | Test Method | EUROSTAR FRANCE/Staramide BG8 |
---|---|---|---|
UL flame retardant rating | 0.75mm | UL 94 | HB |
Limiting Oxygen Index | ISO 4589-2 | 25 % |
physical property | Test Condition | Test Method | EUROSTAR FRANCE/Staramide BG8 |
---|---|---|---|
Shrinkage rate | MD | 内部方法 | 0.15to0.25 % |
density | ISO 1183 | 1.47 g/cm³ |
Thermal performance | Test Condition | Test Method | EUROSTAR FRANCE/Staramide BG8 |
---|---|---|---|
Heat distortion temperature | 1.8MPa,未退火,100mm跨距,HDT | ISO 75-2/Ae | 212 °C |
thermal conductivity | ISO 8302 | 0.33 W/m/K | |
Linear coefficient of thermal expansion | TD:23到60°C | ISO 11359-2 | 8.2E-05 cm/cm/°C |
vicat | ISO 306/B120 | 220 °C | |
Heat distortion temperature | 0.45MPa,未退火,100mm跨距,HDT | ISO 75-2/Be | 224 °C |
Linear coefficient of thermal expansion | MD:23到60°C | ISO 11359-2 | 1.7E-05 cm/cm/°C |