Material Comparison
Product Info
Product Name
Brand Name
Usages
Properties
Certificates

PC DD0009 BK SABIC INNOVATIVE US
LNP™ STAT-KON™
Electrical applications、Casters、household electrical appl
Thermal stability、High gloss
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
Thermal Properties | Test Condition | Test Method | SABIC INNOVATIVE US/DD0009 BK |
---|---|---|---|
Linear thermal expansion coefficient | TD:-40到40°C | ISO11359-2 | 5.7E-05 cm/cm/°C |
Heat Deflection Temperature | 0.45MPa,未退火,3.20mm | ASTMD648 | 141 °C |
Linear thermal expansion coefficient | TD:-40到40°C | ASTME831 | 5.7E-05 cm/cm/°C |
Heat Deflection Temperature | 0.45MPa,Unannealed,64.0mmSpan | ISO75-2/Bf | 139 °C |
Linear thermal expansion coefficient | MD:-40到40°C | ISO11359-2 | 5.4E-05 cm/cm/°C |
Heat Deflection Temperature | 1.8MPa,未退火,3.20mm | ASTMD648 | 133 °C |
1.8MPa,未退火,64.0mm跨距 | ISO75-2/Af | 131 °C | |
Linear thermal expansion coefficient | MD:-40到40°C | ASTME831 | 5.4E-05 cm/cm/°C |
Physical | Test Condition | Test Method | SABIC INNOVATIVE US/DD0009 BK |
---|---|---|---|
Moisture Absorption | 平衡,23°C,50%RH | ISO62 | 0.27 % |
24hr,50%RH | ASTMD570 | 0.18 % | |
Modeling Shrinkage | MD:24小时 | ASTMD955 | 0.80 % |
TD:24hr | ASTMD955 | 0.70 % | |
TD:24小时 | ISO294-4 | 0.72 % | |
MD:24小时 | ISO294-4 | 0.75 % |
Mechanical Properties | Test Condition | Test Method | SABIC INNOVATIVE US/DD0009 BK |
---|---|---|---|
Tensile Strain | 屈服 | ISO527-2 | 4.2 % |
Tensile Elongation | 断裂 | ASTMD638 | 5.6 % |
Flexural Modulus | ASTMD790 | 2830 Mpa | |
Flexural Strength | ASTMD790 | 108 Mpa | |
Tensile Stress | 屈服 | ISO527-2 | 62.8 Mpa |
Tensile Modulus | ISO527-2/1 | 2810 Mpa | |
Tensile Strength | 屈服 | ASTMD638 | 61.9 Mpa |
Flexural Modulus | ISO178 | 2880 Mpa | |
Tensile Elongation | 屈服 | ASTMD638 | 1.2 % |
Tensile Strain | 断裂 | ISO527-2 | 7.5 % |
Tensile Stress | 断裂 | ISO527-2 | 57.1 Mpa |
Flexural Stress | ISO178 | 102 Mpa | |
Tensile Modulus | ASTMD638 | 2830 Mpa | |
Tensile Strength | 断裂 | ASTMD638 | 53.9 Mpa |
Impact Properties | Test Condition | Test Method | SABIC INNOVATIVE US/DD0009 BK |
---|---|---|---|
Instrumented Dart Impact | 23°C,EnergyatPeakLoad | ASTMD3763 | 10.9 J |
23°C | ISO180/1U | 71 kJ/m² | |
Notched Izod Impact Strength | 23°C | ISO180/1A | 6.6 kJ/m² |
Multi-Axial Instrumented Impact Energy | ISO6603-2 | 5.70 J |
Flammability | Test Condition | Test Method | SABIC INNOVATIVE US/DD0009 BK |
---|---|---|---|
Flame Rating | 1.7mm,TestingbySABIC | UL94 | V-0 |
Electrical Properties | Test Condition | Test Method | SABIC INNOVATIVE US/DD0009 BK |
---|---|---|---|
Surface Resistivity | ASTMD257 | 1.0E+4to1.0E+6 ohms |