TPU-Capro Pearlthane® 11T92EM Lubrizol Advanced Materials, Inc.
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
| hardness | Test Condition | Test Method | Lubrizol Advanced Materials, Inc./Pearlthane® 11T92EM |
|---|---|---|---|
| Shore hardness | ShoreA | ASTMD2240 | 91 |
| thermal performance | Test Condition | Test Method | Lubrizol Advanced Materials, Inc./Pearlthane® 11T92EM |
|---|---|---|---|
| Glass transition temperature | ISO 11357-2 | -38.0 °C | |
| Melting temperature | Internal Method | 180to190 °C |
| mechanical properties | Test Condition | Test Method | Lubrizol Advanced Materials, Inc./Pearlthane® 11T92EM |
|---|---|---|---|
| Wear amount | ISO 4649 | 25.0 mm³ |
| Physical properties | Test Condition | Test Method | Lubrizol Advanced Materials, Inc./Pearlthane® 11T92EM |
|---|---|---|---|
| density | 20°C | ISO 2781 | 1.16 g/cm³ |
| -- | ASTM D792 | 1.16 g/cm³ | |
| water content | Internal Method | <0.10 % |
| elastomer | Test Condition | Test Method | Lubrizol Advanced Materials, Inc./Pearlthane® 11T92EM |
|---|---|---|---|
| elongation | Break | ASTMD412 | 600 % |
| Permanent compression deformation | 70°C,22hr | ASTM D395B | 43 % |
| 23°C,70hr | ASTM D395B | 25 % | |
| tear strength | -- | ISO 34-1 | 100 kN/m |
| --1 | ASTM D624 | 100 kN/m | |
| tensile strength | 100%Strain | ASTMD412 | 8.00 MPa |
| Yield | ASTMD412 | 35.0 MPa | |
| 300%Strain | ASTMD412 | 12.0 MPa |