Material Comparison
Product Info
Product Name
Brand Name
Usages
Properties
Certificates

PPS R-4-230BL CPCHEM NETHERLANDS
--
Application in the automotive field
Filler: Glass fiber reinf,40% filler by weight,40% filler by weight
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
| hardness | Test Condition | Test Method | CPCHEM NETHERLANDS/R-4-230BL |
|---|---|---|---|
| Rockwell hardness | M-Sale | ASTM D785 | 104 |
| R-Sale | ASTM D785 | 122 |
| thermal performance | Test Condition | Test Method | CPCHEM NETHERLANDS/R-4-230BL |
|---|---|---|---|
| Hot deformation temperature | 1.8MPa,Unannealed | ASTM D648 | 265 °C |
| Linear coefficient of thermal expansion | MD:100to200°C | ASTME831 | 1.5E-05 cm/cm/°C |
| MD:-50to50°C | ASTME831 | 1.5E-05 cm/cm/°C | |
| TD:-50to50°C | ASTME831 | 4E-05 cm/cm/°C | |
| TD:导热系数 | ASTME831 | 0.31 W/m/K | |
| TD:100to200°C | ASTME831 | 8E-05 cm/cm/°C | |
| UL temperature rating | UL 746B | 200to220 °C |
| mechanical properties | Test Condition | Test Method | CPCHEM NETHERLANDS/R-4-230BL |
|---|---|---|---|
| Bending modulus | ISO 178 | 14000 Mpa | |
| ASTM D790 | 14500 Mpa | ||
| bending strength | ASTM D790 | 221 Mpa | |
| ISO 178 | 210 Mpa | ||
| compressive strength | ASTM D695 | 275 Mpa | |
| elongation | Break | ASTM D638 | 1.2 % |
| Poisson's ratio | 0.43 | ||
| Tensile strain | Break | ISO 527-2 | 1.1 % |
| tensile strength | ASTM D638 | 165 Mpa | |
| ISO 527-2 | 145 Mpa |
| Electrical performance | Test Condition | Test Method | CPCHEM NETHERLANDS/R-4-230BL |
|---|---|---|---|
| Arc resistance | ASTM D495 | 125 sec | |
| Compared to the anti leakage trace index | CTI | UL 746 | PLC 4 |
| Dielectric constant | 25°C,1kHz | ASTM D150 | 3.90 |
| 25°C,1MHz | ASTM D150 | 3.90 | |
| Dielectric strength | ASTM D149 | 20 KV/mm | |
| Dissipation factor | 25°C,1kHz | ASTM D150 | 2E-03 |
| 25°C,1MHz | ASTM D150 | 2E-03 | |
| insulation resistance | 90°C | 1E+12 ohms | |
| Surface resistivity | ASTM D257 | 1E+16 ohms | |
| Volume resistivity | ASTM D257 | 1E+16 ohms·cm |
| Physical properties | Test Condition | Test Method | CPCHEM NETHERLANDS/R-4-230BL |
|---|---|---|---|
| density | ASTM D792 | 1.68 g/cm³ | |
| Shrinkage rate | MD:3.20mm | 0.20 % | |
| TD:3.20mm | 0.50 % | ||
| Water absorption rate | 23°C,24hr | ASTM D570 | 0.020 % |
| impact performance | Test Condition | Test Method | CPCHEM NETHERLANDS/R-4-230BL |
|---|---|---|---|
| Impact strength of cantilever beam gap | ISO 180/A | 8.0 kJ/m² | |
| 3.17mm | ASTM D256 | 80 J/m | |
| Suspended wall beam without notch impact strength | ISO 180 | 20 kJ/m² | |
| 3.18mm | ASTM D4812 | 400 J/m |
| flammability | Test Condition | Test Method | CPCHEM NETHERLANDS/R-4-230BL |
|---|---|---|---|
| Extreme Oxygen Index | ASTM D2863 | 50 % | |
| UL flame retardant rating | 1.6mm | UL 94 | V-05VA |