Material Comparison
Product Info
Product Name
Brand Name
Usages
Properties
Certificates

LCP HA475 BK210P JAPAN POLYPLASTIC
LAPEROS®
Home appliance components,Electrical applications
Low warpage,high strength
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
| thermal performance | Test Condition | Test Method | JAPAN POLYPLASTIC/HA475 BK210P |
|---|---|---|---|
| Hot deformation temperature | 0.45 MPa, Unannealed | ISO 75-2/B | 275 °C |
| 1.8 MPa, Unannealed | ISO 75-2/A | 240 °C |
| mechanical properties | Test Condition | Test Method | JAPAN POLYPLASTIC/HA475 BK210P |
|---|---|---|---|
| Bending modulus | ISO 178 | 12000 Mpa | |
| Bending strain | ISO 178 | 2.5 % | |
| bending strength | ISO 178 | 140 Mpa | |
| elongation | Break | ASTM D638 | 2.1 % |
| tensile strength | ASTM D638 | 110 Mpa |
| Electrical performance | Test Condition | Test Method | JAPAN POLYPLASTIC/HA475 BK210P |
|---|---|---|---|
| Arc resistance | ASTM D495 | 47.0 sec | |
| Compared to the anti leakage trace index | IEC 60112 | V | |
| Dielectric strength | 1.00 mm | IEC 60243-1 | 43 KV/mm |
| 3.00 mm | IEC 60243-1 | 21 KV/mm | |
| Dissipation factor | 1 kHz | IEC 60250 | 0.020 |
| 1 MHz | IEC 60250 | 0.030 | |
| Relative permittivity | 1 MHz | IEC 60250 | 3.50 |
| 1 kHz | IEC 60250 | 4.00 | |
| Volume resistivity | IEC 60093 | 3.0E+16 ohms·cm |
| Physical properties | Test Condition | Test Method | JAPAN POLYPLASTIC/HA475 BK210P |
|---|---|---|---|
| Shrinkage rate | Flow : 1.00 mm | Internal Method | 0.020 % |
| 横向Flow : 1.00 mm | Internal Method | 0.31 % |
| flammability | Test Condition | Test Method | JAPAN POLYPLASTIC/HA475 BK210P |
|---|---|---|---|
| Color number | VF2201/BK210P | ||
| UL flame retardant rating | UL 94 | V-0 |