Material Comparison
Add Comparison Model
Select Products for Comparison (1/4)
Highlight Differences
Hide Same
Product Name / Manufacturer / Model
Grade
Reference Price
| flammability | Test Condition | Test Method | DSM HOLAND/TS271P4 BK |
|---|---|---|---|
| Flammability level | UL 94 | HB | |
| mechanical properties | Test Condition | Test Method | DSM HOLAND/TS271P4 BK |
| Tensile strain | Break | ISO 527-2 | 3.5 % |
| Bending modulus | ISO 178 | 6000 Mpa | |
| tensile strength | Break | ISO 527-2 | 110 Mpa |
| Tensile modulus | ISO 527-2 | 7000 Mpa | |
| Physical properties | Test Condition | Test Method | DSM HOLAND/TS271P4 BK |
| density | ISO 1183 | 1.47 g/cm³ | |
| Water absorption rate | Equilibrium, 23°C, 50% RH | ISO 62 | 2.9 % |
| Shrinkage rate | Flow | ISO 294-4 | 0.90 % |
| 横向Flow | ISO 294-4 | 0.90 % | |
| thermal performance | Test Condition | Test Method | DSM HOLAND/TS271P4 BK |
| RTI Elec | 0.79 mm | UL 746 | 65.0 °C |
| Hot deformation temperature | 1.8 MPa, Unannealed | ISO 75-2/A | 250 °C |
| Melting temperature | ISO 11357-3 | 295 °C | |
| impact performance | Test Condition | Test Method | DSM HOLAND/TS271P4 BK |
| Charpy Notched Impact Strength | 23°C | ISO 179/1eA | 4.0 kJ/m² |