Material Comparison
Product Info
Product Name
Brand Name
Usages
Properties
Certificates

PMMA HI835HS LX MMA KOREA
LGMMA®
Casters、Automotive sector
High impact、Impact resistance
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
Basic performance | Test Condition | Test Method | LX MMA KOREA/HI835HS |
---|---|---|---|
Water absorption | 24h | ASTM D-570 | 0.4 % |
Mechanical properties | Test Condition | Test Method | LX MMA KOREA/HI835HS |
---|---|---|---|
Tensile Elongation | ASTM D-638 | 67 % | |
pulling | ASTM D-638 | 550 kg/cm | |
flexural modulus | ASTM D-790 | 22400 kg/cm | |
bending strength | ASTM D-790 | 870 kg/cm | |
Impact Strength | Izod Notched | ASTM D-256 | 4 kg?cm/cm |
Rockwell hardness | M-Scale | ASTM D-785 | 63 |
Electrical performance | Test Condition | Test Method | LX MMA KOREA/HI835HS |
---|---|---|---|
Dielectric constant | 60Hz | ASTM D-150 | 3.5 |
Anti volume coefficient | ASTM D-257 | >10 Ω.cm | |
power factor | 60Hz | ASTM D-150 | 0.04 |
dielectric strength | 4KV/S | ASTM D-149 | 15 KV/mm |
physical property | Test Condition | Test Method | LX MMA KOREA/HI835HS |
---|---|---|---|
density | ASTM D-792 | 1.17 | |
Transmittance | 3.2mm | ASTM D-1003 | 91 % |
reflective index | ASTM D-542 | 1.49 |
Thermal performance | Test Condition | Test Method | LX MMA KOREA/HI835HS |
---|---|---|---|
Heat Deflection Temperature | 18.6kg | ASTM D-648 | 91 °C |
melt mass-flow rate | 230°C,3.8kg | ASTM D-1238 | 2.6 g/10min |
Coefficient of Linear Thermal Expansion | ASTM D-696 | 6×10 cm/cm/°C | |
specific heat | 0.35 cal/g/°C | ||
Flame Rating | UL94 | HB 1/8",1/16" | |
vicat | 1kg | ASTM D-1525 | 101 °C |
Modeling Shrinkage | ASTM D995-51 | 0.4-0.8 % | |
heat conduction | ASTM D-177 | 5×10 cal/seccm·°C/cm |