Material Comparison
Product Info
Product Name
Brand Name
Usages
Properties
Certificates

EVA 1828 HANWHA KOREA
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
Supplementary Information | Test Condition | Test Method | HANWHA KOREA/1828 |
---|---|---|---|
Processing temperature | Kneader | 90to120 °C | |
RollMill | 90 °C |
hardness | Test Condition | Test Method | HANWHA KOREA/1828 |
---|---|---|---|
Shore hardness | ShoreA,1Sec | ASTM D2240 | 79 |
ShoreD,1Sec | ASTM D2240 | 26 |
thermal performance | Test Condition | Test Method | HANWHA KOREA/1828 |
---|---|---|---|
Brittle temperature | ASTM D746 | <-76.0 °C | |
Melting temperature | ASTM D3417 | 75.0 °C | |
Vicat softening temperature | ASTM D1525 | 44.0 °C |
mechanical properties | Test Condition | Test Method | HANWHA KOREA/1828 |
---|---|---|---|
elongation | Break | ASTM D638 | 800 % |
tensile strength | Break | ASTM D638 | 18.6 Mpa |
Physical properties | Test Condition | Test Method | HANWHA KOREA/1828 |
---|---|---|---|
density | ASTM D1505 | 0.950 g/cm³ | |
melt mass-flow rate | 190°C/2.16kg | ASTM D1238 | 4.0 g/10min |
Vinyl acetate content | Internal Method | 28.0 wt% |