Material Comparison

Product Info
Product Name
Brand Name
Usages
Properties
Certificates
TPE ProvaMed® TPE 1070 ACTEGA GmbH
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--

Plastic Datasheets

hardnessTest ConditionTest MethodACTEGA GmbH/ProvaMed® TPE 1070
Shore hardness邵氏D,5秒ASTM D224018
邵氏A,5秒ASTM D224070
elastomerTest ConditionTest MethodACTEGA GmbH/ProvaMed® TPE 1070
compression set23°C,22hrISO 81520 %
tensile strength 100%应变DIN 535042.40 MPa
compression set70°C,22hrISO 81585 %
tensile strength 屈服DIN 5350410.3 MPa
elongation断裂DIN 535041100 %
compression set100°C,22hrISO 81586 %
physical property Test ConditionTest MethodACTEGA GmbH/ProvaMed® TPE 1070
melt mass-flow rate190°C/5.0kgISO 11337.0 g/10min
densityISO 11830.900 g/cm³
melt mass-flow rate230°C/2.16kgISO 11338.0 g/10min
Thermal performanceTest ConditionTest MethodACTEGA GmbH/ProvaMed® TPE 1070
Glass Transition TemperatureDSC-35.0 °C
melting temperatureDSC163 °C

Contact Us

Get App

Top