Material Comparison

Product Info
Product Name
Brand Name
Usages
Properties
Certificates
TPU E395A KIN JOIN TAIWAN
--
Bottle cap、Electronic field、Electrical field
Low temperature resistanc、Hydrolysis resistance、Antifungal
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--

Plastic Datasheets

Mechanical PropertiesTest ConditionTest MethodKIN JOIN TAIWAN/E395A
Tensile StrengthJIS K-7311450 kg/cm
Tearing Strength120 kg/cm
Compression SetJIS K-630140 %
Tensile ElongationJIS K-7311450 %
Tensile Stress (100%)110 kg/cm
Shore Hardness (Shore A)ASTM D2240/ISO 86895 Shore A
100% SecantASTM D412/ISO 52785 Mpa/Psi
300% Secant150 Mpa/Psi
Tearing StrengthASTM D624/ISO 34120 n/mm²
Shore Hardness (Shore D)ASTM D2240/ISO 86846 Shore D
AbrasionISO 464965 mm³
Taber Abrasion ResistanceJIS K-731145 mg
PhysicalTest ConditionTest MethodKIN JOIN TAIWAN/E395A
hardnessJIS K-731195±3 Shore A
OtherTest ConditionTest MethodKIN JOIN TAIWAN/E395A
Color透明级。
characteristic耐水解,耐霉性,耐低温。聚醚型
Physical PropertiesTest ConditionTest MethodKIN JOIN TAIWAN/E395A
DensityASTM D792/ISO 2781/JIS K73111.13