Material Comparison
Product Info
Product Name
Brand Name
Usages
Properties
Certificates

SPS S930 IDEMITSU JAPAN
XAREC™
Electrical applications、Household daily necessiti
Glass fiber reinforced、High temperature resistan
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
Basic performance | Test Condition | Test Method | IDEMITSU JAPAN/S930 |
---|---|---|---|
Water absorption rate | 24hr | ASTM D-570 | 0.070 % |
Electrical performance | Test Condition | Test Method | IDEMITSU JAPAN/S930 |
---|---|---|---|
Dielectric loss | 1E+6Hz | ASTM D-150 | 0.0020 |
dielectric strength | ASTM D-149 | 36.0 KV/mm | |
dielectric constant | 1E+6Hz | ASTM D-150 | 2.900 |
Volume resistivity | ASTM D-257 | 1E+16 ohm.cm |
Mechanical properties | Test Condition | Test Method | IDEMITSU JAPAN/S930 |
---|---|---|---|
Rockwell hardness | ASTM D-785 | 75 M-scale | |
Flexural modulus | ASTM D-790 | 8500 Mpa | |
bending strength | ASTM D-790 | 150 Mpa | |
tensile strength | ASTM D-638 | 110 Mpa | |
elongation at break | ASTM D-638 | 1.9 % |
physical property | Test Condition | Test Method | IDEMITSU JAPAN/S930 |
---|---|---|---|
Shrinkage rate | Flow | ASTM D-955 | 0.30 % |
Thermal performance | Test Condition | Test Method | IDEMITSU JAPAN/S930 |
---|---|---|---|
Heat distortion temperature | 1.80MPa,未退火,HDT | ASTM D-648 | 235 °C |
0.45MPa,未退火,HDT | ASTM D-648 | 266 °C | |
Linear coefficient of thermal expansion | Flow | ASTM D-696 | 0.000025 cm/cm/℃ |
UL flame retardant rating | UL 94 | V-0 |