PC SABIC INNOVATIVE NANSHA HFD1830 NA9E109T
Light diffusion level
| mechanical properties | Test Condition | Test Method | SABIC INNOVATIVE NANSHA/HFD1830 NA9E109T |
|---|---|---|---|
| bending strength | ISO 178 | 91.0 Mpa | |
| elongation | Break | ASTM D638 | 130 % |
| Bending modulus | 50.0mmSpan | ASTM D790 | 2240 Mpa |
| Tensile modulus | ISO 527-2/1 | 2180 Mpa | |
| ASTM D638 | 2270 Mpa | ||
| tensile strength | Break | ISO 527-2/50 | 56.0 Mpa |
| Yield | ISO 527-2/50 | 63.0 Mpa | |
| Tensile strain | Break | ISO 527-2/50 | 97 % |
| bending strength | Yield,50.0mmSpan | ASTM D790 | 100 Mpa |
| tensile strength | Break | ASTM D638 | 56.0 Mpa |
| Yield | ASTM D638 | 60.0 Mpa | |
| Bending modulus | ISO 178 | 2180 Mpa | |
| Tensile strain | Yield | ISO 527-2/50 | 6.0 % |
| elongation | Yield | ASTM D638 | 5.5 % |
| thermal performance | Test Condition | Test Method | SABIC INNOVATIVE NANSHA/HFD1830 NA9E109T |
| Vicat softening temperature | -- | ISO 306/B50 | 129 °C |
| Hot deformation temperature | 1.8MPa,Unannealed,64.0mmSpan | ISO 75-2/Af | 115 °C |
| 1.8MPa,Unannealed,3.20mm | ASTM D648 | 110 °C | |
| Linear coefficient of thermal expansion | MD:-40to40°C | ISO 11359-2 | 8E-05 cm/cm/°C |
| MD:-40to40°C | ASTME831 | 8E-05 cm/cm/°C | |
| TD:-40to40°C | ASTME831 | 8E-05 cm/cm/°C | |
| RTI Elec | UL 746 | 105 °C | |
| Ball Pressure Test | 125°C | IEC 60695-10-2 | Pass |
| RTI Imp | UL 746 | 105 °C | |
| RTI Str | UL 746 | 105 °C | |
| Vicat softening temperature | ASTM D152510 | 135 °C | |
| -- | ISO 306/B120 | 130 °C | |
| Hot deformation temperature | 0.45MPa,Unannealed,3.20mm | ASTM D648 | 121 °C |
| Linear coefficient of thermal expansion | TD:-40to40°C | ISO 11359-2 | 8E-05 cm/cm/°C |
| flammability | Test Condition | Test Method | SABIC INNOVATIVE NANSHA/HFD1830 NA9E109T |
| UL flame retardant rating | 0.50mm | UL 94 | HB |
| impact performance | Test Condition | Test Method | SABIC INNOVATIVE NANSHA/HFD1830 NA9E109T |
| Charpy Notched Impact Strength | -30°C | ISO 179/1eA | 13 kJ/m² |
| Impact strength of cantilever beam gap | 23°C | ISO 180/1A | 58 kJ/m² |
| Multi axis Instrumented Impact Energy | ISO 6603-2 | 95.0 J | |
| Impact strength of simply supported beam without notch | 23°C | ISO 179/1eU | NoBreak |
| -30°C | ISO 179/1eU | NoBreak | |
| Charpy Notched Impact Strength | 23°C | ISO 179/1eA | 64 kJ/m² |
| Dart impact | 23°C,TotalEnergy | ASTM D3763 | 56.0 J |
| Impact strength of cantilever beam gap | -30°C | ISO 180/1A | 11 kJ/m² |
| Suspended wall beam without notch impact strength | -30°C | ISO 180/1U | NoBreak |
| 23°C | ISO 180/1U | NoBreak | |
| optical performance | Test Condition | Test Method | SABIC INNOVATIVE NANSHA/HFD1830 NA9E109T |
| transmissivity | 2540μm | ASTM D1003 | 88.0 % |
| turbidity | 2540μm | ASTM D1003 | <1.0 % |
| Refractive index | ASTM D542 | 1.582 | |
| Physical properties | Test Condition | Test Method | SABIC INNOVATIVE NANSHA/HFD1830 NA9E109T |
| melt mass-flow rate | 300°C/1.2kg | ASTM D1238 | 40 g/10min |
| Water absorption rate | Equilibrium,23°C,50%RH | ISO 62 | 0.15 % |
| Shrinkage rate | MD:3.20mm | Internal Method | 0.50-0.70 % |
| Water absorption rate | Saturation,23°C | ISO 62 | 0.30 % |
| Melt Volume Flow Rate (MVR) | 300°C/1.2kg | ISO 1133 | 38.0 cm3/10min |
| hardness | Test Condition | Test Method | SABIC INNOVATIVE NANSHA/HFD1830 NA9E109T |
| Rockwell hardness | R-Scale | ASTM D785 | 120 |