POM Copolymer Tarnoform® 500 LS Grupa Azoty ATT Polymers GmbH
--
Applications in the automotive field, thin-walled components
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
| hardness | Test Condition | Test Method | Grupa Azoty ATT Polymers GmbH/Tarnoform® 500 LS |
|---|---|---|---|
| Ball Pressure Test | H358/30 | ISO 2039-1 | 160 MPa |
| Supplementary Information | Test Condition | Test Method | Grupa Azoty ATT Polymers GmbH/Tarnoform® 500 LS |
|---|---|---|---|
| ISOType | ISO 1874 | POM-K.M-GNL.05-002 |
| thermal performance | Test Condition | Test Method | Grupa Azoty ATT Polymers GmbH/Tarnoform® 500 LS |
|---|---|---|---|
| Hot deformation temperature | 1.8MPa,Unannealed | ISO 75-2/A | 115 °C |
| Linear coefficient of thermal expansion | MD:23to55°C | ISO 11359-2 | 1.1E-04 cm/cm/°C |
| Melting temperature | ISO 11357-3 | 167 °C | |
| Short term use temperature | 100 °C | ||
| Vicat softening temperature | ISO 306/B | 150 °C |
| mechanical properties | Test Condition | Test Method | Grupa Azoty ATT Polymers GmbH/Tarnoform® 500 LS |
|---|---|---|---|
| Bending modulus | ISO 178 | 2550 MPa | |
| bending strength | ISO 178 | 65.0 MPa | |
| Tensile modulus | ISO 527-2/1 | 2800 MPa | |
| Tensile strain | Break | ISO 527-2/50 | 20 % |
| Yield | ISO 527-2/50 | 8.0 % | |
| tensile strength | Yield | ISO 527-2/50 | 63.0 MPa |
| Electrical performance | Test Condition | Test Method | Grupa Azoty ATT Polymers GmbH/Tarnoform® 500 LS |
|---|---|---|---|
| Compared to the anti leakage trace index | SolutionA | IEC 60112 | PLC 0 |
| Dielectric constant | 1Hz | IEC 60250 | 3.90 |
| Dielectric strength | 2.00mm | IEC 60243-1 | 25 kV/mm |
| Surface resistivity | IEC 60093 | 1E+14 ohms | |
| Volume resistivity | IEC 60093 | 1E+15 ohms·cm |
| Physical properties | Test Condition | Test Method | Grupa Azoty ATT Polymers GmbH/Tarnoform® 500 LS |
|---|---|---|---|
| density | ISO 1183 | 1.41 g/cm³ | |
| melt mass-flow rate | 190°C/2.16kg | ISO 1133 | 27 g/10min |
| Melt Volume Flow Rate (MVR) | 190°C/2.16kg | ISO 1133 | 23.0 cm³/10min |
| Shrinkage rate | MD:2.00mm | ISO 294-4 | 2.0 % |
| Water absorption rate | Equilibrium,23°C,50%RH | ISO 62 | 0.20 % |
| Saturation,23°C | ISO 62 | 0.80 % |
| impact performance | Test Condition | Test Method | Grupa Azoty ATT Polymers GmbH/Tarnoform® 500 LS |
|---|---|---|---|
| Charpy Notched Impact Strength | -- | ISO 179/1eA | 5.5 kJ/m² |
| -30°C | ISO 179/1eA | 4.5 kJ/m² | |
| Impact strength of cantilever beam gap | ISO 180 | 5.5 kJ/m² | |
| Impact strength of simply supported beam without notch | -30°C | ISO 179/1eU | 110 kJ/m² |
| -- | ISO 179/1eU | 140 kJ/m² |
| flammability | Test Condition | Test Method | Grupa Azoty ATT Polymers GmbH/Tarnoform® 500 LS |
|---|---|---|---|
| Burning rate | FMVSS302 | <100 mm/min | |
| UL flame retardant rating | 3.2mm | UL 94 | HB |