POM 500TL DUPONT JAPAN
Delrin® 
Bottle cap、Electrical appliances、Fitness equipment
High sliding、Aging resistance、wear resistant
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--

Plastic Datasheets

Impact resistanceTest ConditionTest MethodDUPONT JAPAN/500TL
Charpy Notched Impact Strength23°CISO179/1eA13 kJ/m²
Impact strength of cantilever beam gap23°CISO180/1A12 kJ/m²
Charpy Notched Impact Strength-30°CISO179/1eA7.0 kJ/m²
Impact strength of cantilever beam gap-40°CISO180/1A9.0 kJ/m²
Supplementary InformationTest ConditionTest MethodDUPONT JAPAN/500TL
EmissionVDA275<8.00 mg/kg
Emissions of Organic CompoundsVDA2773.40 µgC/g
Mechanical propertiesTest ConditionTest MethodDUPONT JAPAN/500TL
Nominal tensile fracture strainISO527-228 %
Bending stress3.5%应变ISO17860.0 Mpa
Tensile stress屈服ISO527-254.0 Mpa
Tensile strain屈服ISO527-217 %
Tensile modulusISO527-22300 Mpa
Flexural modulusISO1782000 Mpa
flammabilityTest ConditionTest MethodDUPONT JAPAN/500TL
UL flame retardant rating0.75mmUL94HB
1.5mmUL94HB
FMVSS flammabilityFMVSS302B
Burning rate 31.00mmISO379555 mm/min
UL flame retardant rating0.75mmIEC60695-11-10,-20HB
1.5mmIEC60695-11-10,-20HB
Fogging-G-valuecondensateISO64522E-04 g
physical property Test ConditionTest MethodDUPONT JAPAN/500TL
Shrinkage rateTDISO294-41.5 %
melt mass-flow rate190°C/2.16kgISO113312 g/10min
MediumDensity1.19 g/cm³
Shrinkage rateMDISO294-41.5 %
densityISO11831.39 g/cm³
Thermal performanceTest ConditionTest MethodDUPONT JAPAN/500TL
AnnealingTemperature160 °C
melting temperatureISO11357-3178 °C
AnnealingTime-Optional30.0 min/mm
Heat distortion temperature1.8MPa,未退火ISO75-2/A76.0 °C
0.45MPa,未退火ISO75-2/B146 °C