Material Comparison
Product Info
Product Name
Brand Name
Usages
Properties
Certificates

PC DFL34-BK1A657L SABIC INNOVATIVE US
LNP™ LUBRICOMP™
Electronic and Electrical、Lighting applications
Easy to form、Easy to demould
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
Impact resistance | Test Condition | Test Method | SABIC INNOVATIVE US/DFL34-BK1A657L |
---|---|---|---|
23°C | ISO 180/1A | 14 kJ/m² | |
ISO 180/1U | 49 kJ/m² | ||
ASTM D256 | 150 J/m | ||
ASTM D4812 | 740 J/m | ||
23°C,TotalEnergy | ASTM D3763 | 19.6 J |
Mechanical properties | Test Condition | Test Method | SABIC INNOVATIVE US/DFL34-BK1A657L |
---|---|---|---|
fracture | ISO 527-2/5 | 93.0 Mpa | |
Wear factor | Washer | ASTM D3702Modified | 89.0 10^-10in^5-min/ft-lb-hr |
yield | ISO 527-2/5 | 2.8 % | |
fracture | ASTM D638 | 95.0 Mpa | |
ASTM D638 | 2.7 % | ||
coefficient of friction | 与自身-动态 | ASTM D3702Modified | 0.46 |
与自身-静态 | ASTM D3702Modified | 0.50 | |
--5 | ISO 178 | 6200 Mpa | |
Wear factor | Ring | ASTM D3702Modified | 13.0 10^-10in^5-min/ft-lb-hr |
50.0mm span | ASTM D790 | 6320 Mpa | |
--1 | ASTM D638 | 7190 Mpa | |
fracture | ISO 527-2/5 | 3.1 % | |
Fracture, 50.0mm span | ASTM D790 | 145 Mpa |
physical property | Test Condition | Test Method | SABIC INNOVATIVE US/DFL34-BK1A657L |
---|---|---|---|
24hr,50%RH | ASTM D570 | 0.090 % | |
Shrinkage rate | TD:24小时 | ASTM D955 | 0.20-0.40 % |
MD:24小时 | ASTM D955 | 0.020-0.040 % | |
Balance, 23 ° C, 50% RH | ISO 62 | 0.13 % |
Thermal performance | Test Condition | Test Method | SABIC INNOVATIVE US/DFL34-BK1A657L |
---|---|---|---|
Linear coefficient of thermal expansion | MD:-30到30°C | ASTM D696 | 3.7E-05 cm/cm/°C |
0.45MPa, Unanealed, 64.0mm span | ISO 75-2/Bf | 146 °C | |
1.8MPa, Unanealed, 64.0mm span | ISO 75-2/Af | 141 °C | |
Linear coefficient of thermal expansion | TD:-30到30°C | ASTM D696 | 6.3E-05 cm/cm/°C |
1.8MPa, Unanealed, 3.20mm | ASTM D648 | 142 °C | |
0.45MPa, Unanealed, 3.20mm | ASTM D648 | 146 °C |