Material Comparison

Product Info
Product Name
Brand Name
Usages
Properties
Certificates
TPE STARGUM P 702 naturale Daloga srl
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--

Plastic Datasheets

Supplementary InformationTest ConditionTest MethodDaloga srl/STARGUM P 702 naturale
Resistance Against SaponificationHD22.10S1<200 mgKOH/g
hardnessTest ConditionTest MethodDaloga srl/STARGUM P 702 naturale
Shore hardness邵氏A,30秒ISO 86884to88
Mechanical propertiesTest ConditionTest MethodDaloga srl/STARGUM P 702 naturale
wear resistanceDIN 5351637.0to47.0 mm³
Tensile strain断裂ISO 527-2580to700 %
tensile strength 屈服ISO 527-232.4to39.6 MPa
Electrical performanceTest ConditionTest MethodDaloga srl/STARGUM P 702 naturale
Volume resistivity20°CASTM D257>5.0E+13 ohms·cm
flammabilityTest ConditionTest MethodDaloga srl/STARGUM P 702 naturale
Limiting Oxygen IndexISO 4589-226to29 %
physical property Test ConditionTest MethodDaloga srl/STARGUM P 702 naturale
densityISO 11831.26to1.30 g/cm³
agingTest ConditionTest MethodDaloga srl/STARGUM P 702 naturale
Change rate of ultimate elongation in air100°C,168hrUL 1581<-30 %
Change rate of tensile strength in air90°C,168hr,在ASTM#2油中UL 1581<-30 %
Change rate of ultimate elongation in air121°C,18hr,在ASTM#2油中UL 1581<-30 %
Change rate of tensile strength in air121°C,18hr,在ASTM#2油中UL 1581<-30 %
Change rate of ultimate elongation in air90°C,168hr,在ASTM#2油中UL 1581<-30 %
Change rate of tensile strength in air100°C,168hrUL 1581<-30 %
elastomerTest ConditionTest MethodDaloga srl/STARGUM P 702 naturale
tear strengthDIN 5351577.0to87.0 kN/m
Thermal performanceTest ConditionTest MethodDaloga srl/STARGUM P 702 naturale
brittle temperatureISO 458-43.0--39.0 °C
thermal stabilityISO R182>80

Contact Us

Get App

Top