Supplementary Information | Test Condition | Test Method | LOTTE KOREA/SFC-750M |
---|---|---|---|
HeatSealTemperature | 30.0µm | 内部方法 | 122 °C |
hardness | Test Condition | Test Method | LOTTE KOREA/SFC-750M |
---|---|---|---|
Rockwell hardness | R计秤 | ISO 2039-2 | 77 |
R级 | ASTM D785 | 77 |
Mechanical properties | Test Condition | Test Method | LOTTE KOREA/SFC-750M |
---|---|---|---|
elongation | 断裂 | ASTMD638 | >500 % |
Flexural modulus | ASTMD790 | 735 Mpa | |
tensile strength | 屈服 | ASTMD638 | 22.6 Mpa |
coefficient of friction | 铸造薄膜 | 内部方法 | <1.0 |
optical performance | Test Condition | Test Method | LOTTE KOREA/SFC-750M |
---|---|---|---|
Haze ratio | 30.0µm,铸造薄膜 | ASTM D1003 | <2.0 % |
physical property | Test Condition | Test Method | LOTTE KOREA/SFC-750M |
---|---|---|---|
melt mass-flow rate | 230°C/2.16kg | ASTMD1238 | 7.0 g/10min |
Thermal performance | Test Condition | Test Method | LOTTE KOREA/SFC-750M |
---|---|---|---|
Heat distortion temperature | 0.45MPa,未退火,HDT | ASTMD648 | 75.0 °C |
melting temperature | 内部方法,ASTMD3418 | 130 °C |