Material Comparison
Add Comparison Model
Select Products for Comparison (1/4)
Highlight Differences
Hide Same
Product Name / Manufacturer / Model
Grade
Certificates
Reference Price
| thermal performance | Test Condition | Test Method | EXXONMOBIL FRANCE/AP03B |
|---|---|---|---|
| Hot deformation temperature | 0.45MPa,Annealed | ASTM D648 | 119 °C |
| 0.45MPa,Unannealed | ASTM D648 | 105 °C | |
| 1.8MPa,Unannealed | ISO 75-2/A | 54.6 °C | |
| 0.45MPa,Unannealed | ISO 75-2/Bf | 93.5 °C | |
| mechanical properties | Test Condition | Test Method | EXXONMOBIL FRANCE/AP03B |
| tensile strength | Yield3 | ASTM D638 | 26.6 Mpa |
| Yield | ISO 527-2/50 | 25.1 Mpa | |
| Bending modulus | 1%Secant5 | ASTM D790B | 1500 Mpa |
| elongation | Yield3 | ASTM D638 | 5.0 % |
| Yield | ISO 527-2/50 | 4.9 % | |
| Bending modulus | --6 | ISO 178 | 1260 Mpa |
| 1%Secant4 | ASTM D542 | 1310 Mpa | |
| Tensile modulus | ISO 527-2/1 | 1440 Mpa | |
| impact performance | Test Condition | Test Method | EXXONMOBIL FRANCE/AP03B |
| Dart impact | -29°C,3.18mm | ASTM D5420 | 17.3 J |
| hardness | Test Condition | Test Method | EXXONMOBIL FRANCE/AP03B |
| Rockwell hardness | ASTM D785 | 95 | |
| Physical properties | Test Condition | Test Method | EXXONMOBIL FRANCE/AP03B |
| melt mass-flow rate | 230°C/2.16kg | ASTM D1238 | 30 g/10min |