Material Comparison
Product Info
Product Name
Brand Name
Usages
Properties
Certificates

PA6 TechnoMid PA6 S GF 50 HY TECHNOCOMPOUND GERMANY
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
Impact resistance | Test Condition | Test Method | TECHNOCOMPOUND GERMANY/TechnoMid PA6 S GF 50 HY |
---|---|---|---|
Charpy Notched Impact Strength | 23°C | ISO 179/1eA | 15 kJ/m² |
-30°C | ISO 179/1eA | 11 kJ/m² | |
Impact strength of simply supported beam without notch | 23°C | ISO 179/1eU | 90 kJ/m² |
-30°C | ISO 179/1eU | 85 kJ/m² |
hardness | Test Condition | Test Method | TECHNOCOMPOUND GERMANY/TechnoMid PA6 S GF 50 HY |
---|---|---|---|
ball-indentation hardness | ISO 2039-1 | 270 MPa |
Electrical performance | Test Condition | Test Method | TECHNOCOMPOUND GERMANY/TechnoMid PA6 S GF 50 HY |
---|---|---|---|
relative permittivity | 1MHz | IEC 60250 | 3.80 |
dielectric strength | 1.00mm | IEC 60243-1 | 36 kV/mm |
Mechanical properties | Test Condition | Test Method | TECHNOCOMPOUND GERMANY/TechnoMid PA6 S GF 50 HY |
---|---|---|---|
tensile strength | 断裂 | ISO 527-2/5 | 210 MPa |
Tensile strain | 断裂 | ISO 527-2/5 | 2.5 % |
屈服 | ISO 527-2/50 | 2.5 % | |
Tensile modulus | ISO 527-2/1 | 16000 MPa | |
tensile strength | 屈服 | ISO 527-2/50 | 210 MPa |
flammability | Test Condition | Test Method | TECHNOCOMPOUND GERMANY/TechnoMid PA6 S GF 50 HY |
---|---|---|---|
UL flame retardant rating | 0.8mm | UL 94 | HB |
physical property | Test Condition | Test Method | TECHNOCOMPOUND GERMANY/TechnoMid PA6 S GF 50 HY |
---|---|---|---|
Shrinkage rate | TD | ISO 294-4 | 0.50 % |
viscosity number | ISO 307 | 150 cm³/g | |
Shrinkage rate | MD | ISO 294-4 | 0.050 % |
Water absorption rate | 平衡,23°C,50%RH | ISO 62 | 1.5 % |
饱和,23°C | ISO 62 | 4.8 % | |
density | ISO 1183 | 1.55 g/cm³ |
Thermal performance | Test Condition | Test Method | TECHNOCOMPOUND GERMANY/TechnoMid PA6 S GF 50 HY |
---|---|---|---|
melting temperature | ISO 11357-3 | 220 °C | |
Linear coefficient of thermal expansion | TD:23到80°C | ISO 11359-2 | 9.0E-5到1.1E-4 cm/cm/°C |
Heat distortion temperature | 0.45MPa,未退火,HDT | ISO 75-2/B | 220 °C |
1.8MPa,未退火,HDT | ISO 75-2/A | 210 °C | |
Linear coefficient of thermal expansion | MD:23到80°C | ISO 11359-2 | 1.0E-5到2.5E-5 cm/cm/°C |
Heat distortion temperature | 8.0MPa,未退火,HDT | ISO 75-2/C | 170 °C |