PA6 6B30 300 NC DOMO CHEM GERMANY
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
| thermal performance | Test Condition | Test Method | DOMO CHEM GERMANY/6B30 300 NC |
|---|---|---|---|
| Melting temperature | ISO 11357-3 | 221 °C |
| mechanical properties | Test Condition | Test Method | DOMO CHEM GERMANY/6B30 300 NC |
|---|---|---|---|
| Tensile modulus | ISO 527-2/1 | 4200 Mpa | |
| Tensile strain | Break | ISO 527-2/50 | 14 % |
| tensile strength | Break | ISO 527-2/50 | 75.0 Mpa |
| Physical properties | Test Condition | Test Method | DOMO CHEM GERMANY/6B30 300 NC |
|---|---|---|---|
| Melt Volume Flow Rate (MVR) | 275°C/5.0 kg | ISO 1133 | 100 cm3/10min |
| Shrinkage rate | 横向Flow : 23°C, 72hr | ISO 2577 | 1.1 - 1.3 % |
| Flow : 23°C, 72hr | ISO 2577 | 1.0 - 1.2 % | |
| Stickiness | 96% H2SO4 | ISO 307 | 145 cm³/g |
| impact performance | Test Condition | Test Method | DOMO CHEM GERMANY/6B30 300 NC |
|---|---|---|---|
| Impact strength of simply supported beam without notch | 23°C | ISO 179/1eU | 45 kJ/m² |
| flammability | Test Condition | Test Method | DOMO CHEM GERMANY/6B30 300 NC |
|---|---|---|---|
| Burning rate | FMVSS 302 | < 100 mm/min |
| injection | Test Condition | Test Method | DOMO CHEM GERMANY/6B30 300 NC |
|---|---|---|---|
| drying temperature | 75 to 85 °C | ||
| drying time | 2.0 to 4.0 hr | ||
| Mold temperature | 60 to 80 °C | ||
| Processing (melt) temperature | 240 to 280 °C |