PTFE M112(微粉) DAIKIN JAPAN
POLYFLON™
--
--
UL
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
| thermal performance | Test Condition | Test Method | DAIKIN JAPAN/M112(微粉) |
|---|---|---|---|
| Vicat softening temperature | 连续使用温度 | 260 °C | |
| Melting Temperature | DSC | 323 °C |
| flame retardant performance | Test Condition | Test Method | DAIKIN JAPAN/M112(微粉) |
|---|---|---|---|
| UL flame retardant rating | UL -94 | V-0 0.067mm | |
| UL -94 | V-0 0.75mm |
| mechanical properties | Test Condition | Test Method | DAIKIN JAPAN/M112(微粉) |
|---|---|---|---|
| Elongation at Break | 受载变形 | ASTM D621 | 12.9 % |
| 23°C | ASTM D638 | 430 % | |
| 压缩形变 | ASTM D621 | 8.7 % | |
| 抗压强度 | ASTM D695 | 7.7 Mpa | |
| tensile strength | 23°C | ASTM D638 | 40 Mpa |
| Electrical performance | Test Condition | Test Method | DAIKIN JAPAN/M112(微粉) |
|---|---|---|---|
| Dielectric constant | ASTM D150 | <2.10 1kHz | |
| Dielectric strength | ASTM D149 | 3300 KV/mm | |
| Dissipation factor | ASTM D150 | <1.0E-4 | |
| Surface resistivity | ASTM D257 | >1.0E+15 Ω.cm | |
| Volume resistivity | ASTM D257 | >1.0E+18 Ω.cm |
| Physical properties | Test Condition | Test Method | DAIKIN JAPAN/M112(微粉) |
|---|---|---|---|
| Shrinkage rate | MIT弯曲的寿命 | ASTM D2178 | 2.7E+07 |
| 堆积密度 | ASTM D4894 | 0.36 g/cm³ | |
| MD | ASTM D995 | 0.046 % | |
| 拉伸空隙指数 | ASTM D4895 | 40.0 |