PA66 Wellamid® GFT1675-N1 WELLAMID USA
--
--
Filler, glass fiber reinforced material, 33%, filler by weight
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--

Plastic Datasheets

Impact resistanceTest ConditionTest MethodWELLAMID USA/Wellamid® GFT1675-N1
Impact strength of cantilever beam gap23°CISO 18020 kJ/m²
Mechanical propertiesTest ConditionTest MethodWELLAMID USA/Wellamid® GFT1675-N1
Flexural modulus23°CISO 1787900 MPa
tensile strength 屈服,23°CISO 527-2145 MPa
Tensile strain屈服,23°CISO 527-23.0 %
bending strength23°CISO 178190 MPa
physical property Test ConditionTest MethodWELLAMID USA/Wellamid® GFT1675-N1
Shrinkage rateTD:23°CISO 294-40.80to1.2 %
MD:23°CISO 294-40.30to0.70 %
densityISO 11831.34 g/cm³
Thermal performanceTest ConditionTest MethodWELLAMID USA/Wellamid® GFT1675-N1
Heat distortion temperature1.8MPa,未退火,HDTISO 75-2/A245 °C
melting temperatureISO 3146260 °C