Material Comparison
Add Comparison Model
Select Products for Comparison (1/4)
Highlight Differences
Hide Same
Product Name / Manufacturer / Model
Grade
Reference Price
| mechanical properties | Test Condition | Test Method | DSM HOLAND/HF4130 |
|---|---|---|---|
| tensile strength | Break, 120°C | ISO 527-2 | 125 Mpa |
| Break, 180°C | ISO 527-2 | 95.0 Mpa | |
| Break, 160°C | ISO 527-2 | 110 Mpa | |
| Tensile strain | Break, 160°C | ISO 527-2 | 5.5 % |
| Break, 180°C | ISO 527-2 | 5.5 % | |
| Break | ISO 527-2 | 3.0 % | |
| tensile strength | Break | ISO 527-2 | 210 Mpa |
| Tensile modulus | -- | ISO 527-2 | 10000 Mpa |
| 180°C | ISO 527-2 | 4700 Mpa | |
| 200°C | ISO 527-2 | 4500 Mpa | |
| Bending modulus | ISO 178 | 9000 Mpa | |
| Tensile strain | Break, 120°C | ISO 527-2 | 5.5 % |
| Tensile modulus | 120°C | ISO 527-2 | 5500 Mpa |
| 160°C | ISO 527-2 | 5000 Mpa | |
| Tensile strain | Break, 200°C | ISO 527-2 | 5.5 % |
| tensile strength | Break, 200°C | ISO 527-2 | 90.0 Mpa |
| thermal performance | Test Condition | Test Method | DSM HOLAND/HF4130 |
| Linear coefficient of thermal expansion | Across Flow | ISO 11359-2 | 6.0E-5 cm/cm/°C |
| Hot deformation temperature | 0.45 MPa, Unannealed | ISO 75-2/B | 290 °C |
| 1.8 MPa, Unannealed | ISO 75-2/A | 290 °C | |
| RTI Elec | UL 746 | 65.0 °C | |
| Linear coefficient of thermal expansion | Flow | ISO 11359-2 | 2.5E-5 cm/cm/°C |
| Thermal Index - 5000 hr | IEC 60216 | 177 °C | |
| Melting temperature | ISO 11357-3 | 295 °C | |
| Physical properties | Test Condition | Test Method | DSM HOLAND/HF4130 |
| Water absorption rate | Equilibrium, 23°C, 50% RH | ISO 62 | 2.6 % |
| Shrinkage rate | Flow | ISO 294-4 | 0.50 % |
| 横向Flow | ISO 294-4 | 1.3 % | |
| impact performance | Test Condition | Test Method | DSM HOLAND/HF4130 |
| Impact strength of simply supported beam without notch | 23°C | ISO 179/1eU | 60 kJ/m² |
| -30°C | ISO 179/1eU | 60 kJ/m² | |
| flammability | Test Condition | Test Method | DSM HOLAND/HF4130 |
| Flammability level | UL 94 | HB |