POM UR304 KOLON KOREA
KOCETAL® 
switch,Fasteners
High impact resistance,Low odor and no taste
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--

Plastic Datasheets

Impact resistanceTest ConditionTest MethodKOLON KOREA/UR304
Charpy Notched Impact Strength23°CISO 179/1eA13 kJ/m²
Impact strength of cantilever beam gap23°CASTM D256130 J/m
hardnessTest ConditionTest MethodKOLON KOREA/UR304
Rockwell hardnessM级ASTM D78576
M计秤ISO 2039-283
Electrical performanceTest ConditionTest MethodKOLON KOREA/UR304
Volume resistivityASTMD2571E+14 ohms·cm
Dissipation Factor1MHzASTM D1506E-03
dielectric strengthASTMD14919 KV/mm
dielectric constantASTM D1503.70
Surface ResistivityASTMD2571E+16 ohms
Mechanical propertiesTest ConditionTest MethodKOLON KOREA/UR304
elongation断裂,23°CISO 527-2>50 %
bending strength23°CISO 17855.0 Mpa
Flexural modulus23°CISO 1781900 Mpa
bending strength23°CASTM D79060.0 Mpa
tensile strength 屈服,23°CASTM D63845.0 Mpa
elongation屈服,23°CASTM D638140 %
Flexural modulus23°CASTM D7901800 Mpa
tensile strength 23°CISO 527-245.0 Mpa
flammabilityTest ConditionTest MethodKOLON KOREA/UR304
UL flame retardant rating0.8mmUL 94HB
physical property Test ConditionTest MethodKOLON KOREA/UR304
Shrinkage rateMDASTM D9551.7 %
TDISO 294-42.2 %
MDISO 294-42.0 %
Water absorption rate23°C,24hrISO 620.63 %
densityASTMD7921.36 g/cm³
Water absorption rate平衡,23°C,60%RHASTM D5700.25 %
melt mass-flow rate190°C/2.16kgASTM D123812 g/10min
190°C/2.16kgISO 11337.5 g/10min
Thermal performanceTest ConditionTest MethodKOLON KOREA/UR304
Heat distortion temperature1.8MPa,未退火,HDTASTM D64882.0 °C
melting temperatureISO 11357-3166 °C
Heat distortion temperature0.45MPa,未退火,HDTASTM D648145 °C
1.8MPa,未退火,HDTISO 75-2/A72.0 °C
Linear coefficient of thermal expansionMDASTM D6961.3E-04 cm/cm/°C