Material Comparison
Product Info
Product Name
Brand Name
Usages
Properties
Certificates

PA12 4533 SA01 MED ARKEMA FRANCE
--
Medical and nursing suppl
Low wear
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
Impact resistance | Test Condition | Test Method | ARKEMA FRANCE/4533 SA01 MED |
---|---|---|---|
Impact strength of simply supported beam without notch | -30°C | ISO 179/1eU | -- |
23°C | ISO 179/1eU | -- |
hardness | Test Condition | Test Method | ARKEMA FRANCE/4533 SA01 MED |
---|---|---|---|
Shore hardness | 邵氏 D, 15 秒 | ISO 7619-1 | 41 |
邵氏 A, 3 秒 | ISO 7619-1 | 92 |
Mechanical properties | Test Condition | Test Method | ARKEMA FRANCE/4533 SA01 MED |
---|---|---|---|
Tensile modulus | ISO 527-2 | 88.0 Mpa | |
Tensile strain | 断裂 | ISO 527-2 | > 50 % |
tensile strength | 50% 应变 | ISO 527-2 | 9.00 Mpa |
squeeze out | Test Condition | Test Method | ARKEMA FRANCE/4533 SA01 MED |
---|---|---|---|
drying temperature | 60 to 70 °C | ||
Melt Temperature | 210 to 230 °C | ||
drying time | 4.0 to 6.0 hr |
physical property | Test Condition | Test Method | ARKEMA FRANCE/4533 SA01 MED |
---|---|---|---|
Water absorption rate | 平衡, 23°C, 50% RH | ISO 62 | 0.40 % |
Shrinkage rate | 流量 | ISO 294-4 | 1.1 % |
Water absorption rate | 饱和, 23°C | ISO 62 | 1.2 % |
Shrinkage rate | 横向流量 | ISO 294-4 | 0.40 % |
Thermal performance | Test Condition | Test Method | ARKEMA FRANCE/4533 SA01 MED |
---|---|---|---|
melting temperature | ISO 11357-3 | 147 °C | |
vicat | ISO 306/B50 | 111 °C |
injection | Test Condition | Test Method | ARKEMA FRANCE/4533 SA01 MED |
---|---|---|---|
drying time | 4.0 to 6.0 hr | ||
Processing (melt) temperature | 200 to 270 °C | ||
drying temperature | 60 to 70 °C | ||
Temperature | 10 to 30 °C |