PA66 GERMAMID B 6.6 GF 30 HY Kunststoff-Kontor-Hamburg GmbH
--
--
Filler, glass fiber reinforced material, 30%, filler by weight
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
Impact resistance | Test Condition | Test Method | Kunststoff-Kontor-Hamburg GmbH/GERMAMID B 6.6 GF 30 HY |
---|---|---|---|
Impact strength of simply supported beam without notch | ISO 179/1eU | 35 kJ/m² | |
Charpy Notched Impact Strength | ISO 179/1eA | 8.0 kJ/m² |
Electrical performance | Test Condition | Test Method | Kunststoff-Kontor-Hamburg GmbH/GERMAMID B 6.6 GF 30 HY |
---|---|---|---|
Surface Resistivity | IEC 60093 | 1E+13 ohms |
Mechanical properties | Test Condition | Test Method | Kunststoff-Kontor-Hamburg GmbH/GERMAMID B 6.6 GF 30 HY |
---|---|---|---|
Tensile modulus | ISO 527-2 | 10000 MPa | |
Tensile strain | 断裂 | ISO 527-2 | 2.5 % |
tensile strength | 屈服 | ISO 527-2 | 165 MPa |
physical property | Test Condition | Test Method | Kunststoff-Kontor-Hamburg GmbH/GERMAMID B 6.6 GF 30 HY |
---|---|---|---|
Shrinkage rate | ISO 294-4 | 0.30to0.80 % | |
Water absorption rate | 饱和,23°C | ISO 62 | 2.0 % |
density | ISO 1183 | 1.36 g/cm³ |
Thermal performance | Test Condition | Test Method | Kunststoff-Kontor-Hamburg GmbH/GERMAMID B 6.6 GF 30 HY |
---|---|---|---|
thermal conductivity | ISO 8302 | 0.24 W/m/K | |
Heat distortion temperature | 1.8MPa,未退火,HDT | ISO 75-2/A | 250 °C |
melting temperature | 255 °C |