| elastomer | Test Condition | Test Method | KRAIBURG TPE GERMANY/M TM5MED |
|---|---|---|---|
| Permanent compression deformation | 100°C,24hr | ISO 815 | 46 % |
| tensile strength | Yield | ISO 37 | 10.0 Mpa |
| elongation | Break | ISO 37 | 850 % |
| tear strength | ISO 34-1 | 15 kN/m | |
| Permanent compression deformation | 70°C,24hr | ISO 815 | 32 % |
| 23°C,72hr | ISO 815 | 19 % | |
| hardness | Test Condition | Test Method | KRAIBURG TPE GERMANY/M TM5MED |
| Shore hardness | ShoreA | ISO 7619 | 46 |