plas
Log In

Material Comparison

Product Info
Product Name
Brand Name
Usages
Properties
Certificates
PUR-Ether//TDI Andur 93-AP USA Anderson Development
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--

Plastic Datasheets

hardnessTest ConditionTest MethodUSA Anderson Development/Andur 93-AP
Shore hardnessShoreAASTM D224092
mechanical propertiesTest ConditionTest MethodUSA Anderson Development/Andur 93-AP
elongationYieldASTM D638450 %
tensile strengthYieldASTM D63842.1 MPa
thermosettingTest ConditionTest MethodUSA Anderson Development/Andur 93-AP
storage stability70°C4.0to6.0 min
Thermosetting mixed viscosity70°CASTM D2393880 cP
Physical propertiesTest ConditionTest MethodUSA Anderson Development/Andur 93-AP
Apparent densityASTM D18951.06 g/cm³
Shrinkage rateMDASTM D9551.7 %
elastomerTest ConditionTest MethodUSA Anderson Development/Andur 93-AP
Permanent compression deformationASTM D39526 %
tensile strength300%StrainASTM D41221.3 MPa
200%StrainASTM D41215.9 MPa
100%StrainASTM D41211.7 MPa