Material Comparison
Product Info
Product Name
Brand Name
Usages
Properties
Certificates

Plastomer, Ethylene-based Filter-bond™ R-36 HAPCO USA
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
Impact resistance | Test Condition | Test Method | HAPCO USA/Filter-bond™ R-36 |
---|---|---|---|
Impact strength of cantilever beam gap | ASTM D256 | 24 J/m |
Supplementary Information | Test Condition | Test Method | HAPCO USA/Filter-bond™ R-36 |
---|---|---|---|
CureTime | 21°C | 内部方法 | 1.0 day |
hardness | Test Condition | Test Method | HAPCO USA/Filter-bond™ R-36 |
---|---|---|---|
Shore hardness | 邵氏D | ASTM D2240 | 80 |
Mechanical properties | Test Condition | Test Method | HAPCO USA/Filter-bond™ R-36 |
---|---|---|---|
elongation | 断裂 | ASTM D638 | 7.5 % |
Tensile modulus | ASTM D638 | 2000 MPa | |
Flexural modulus | ASTM D790 | 1760 MPa | |
tensile strength | 屈服 | ASTM D638 | 56.9 MPa |
bending strength | ASTM D790 | 94.8 MPa |
thermosetting | Test Condition | Test Method | HAPCO USA/Filter-bond™ R-36 |
---|---|---|---|
Thermosetting mixed viscosity | 25°C | ASTM D4878 | 15000to23000 cP |
GelTime | 25°C | ASTM D2971 | 2.0 hr |
Thermosetting components | 部件A | 按重量计算的混合比:100.按容量计算的混合比:100 | |
部件B | 按重量计算的混合比:50.按容量计算的混合比:46 |
physical property | Test Condition | Test Method | HAPCO USA/Filter-bond™ R-36 |
---|---|---|---|
Shrinkage rate | MD | ASTM D2566 | 0.050to0.20 % |
density | ASTM D4669 | 1.10 g/cm³ | |
Weight Percubicinch | 18 g |
Thermal performance | Test Condition | Test Method | HAPCO USA/Filter-bond™ R-36 |
---|---|---|---|
Heat distortion temperature | HDT | ASTM D648 | 7562 °C |