| Physical properties | Test Condition | Test Method | KURARAY JAPAN/SP292B |
|---|---|---|---|
| melt mass-flow rate | 210℃/2.16 kg | ISO 1133 | 4.5 g/10 min |
| 190℃/2.16 kg | ISO 1133 | 2.2 g/10 min | |
| mechanical properties | Test Condition | Test Method | KURARAY JAPAN/SP292B |
| tensile strength | Break | ISO 527-2 | 25.0 Mpa |
| Tensile modulus | ISO 527-2 | 2000 Mpa | |
| Tensile strain | Break | ISO 527-2 | 14 % |
| thermal performance | Test Condition | Test Method | KURARAY JAPAN/SP292B |
| Melting temperature | ISO 3146 | 163 °C | |
| Glass transition temperature | DSC | DSC | 43.0 °C |