PC 1800 COVESTRO GERMANY
Makrolon®
Electrical applications,Automotive Applications,Laptop case
Thermal stability,High temperature resistan,high viscosity
UL
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
| Other performance | Test Condition | Test Method | COVESTRO GERMANY/1800 |
|---|---|---|---|
| Extreme Oxygen Index | ISO 4589 | 24 % |
| machinability | Test Condition | Test Method | COVESTRO GERMANY/1800 |
|---|---|---|---|
| Injection temperature | ISO 294 | 200 mm/g | |
| Melt Temperature | ISO 294 | 330 °C | |
| Mold temperature | ISO 294 | 100 °C |
| thermal performance | Test Condition | Test Method | COVESTRO GERMANY/1800 |
|---|---|---|---|
| Hot deformation temperature | 1.80Mpa | ISO 75-1 | 162/151/160 °C |
| Linear thermal expansion coefficient in flow direction | 23~55℃ | ASTME811 | 0.7 10 |
| Linear thermal expansion coefficient in the vertical flow direction | 23~55℃ | ASTME811 | 0.7 10 |
| mechanical properties | Test Condition | Test Method | COVESTRO GERMANY/1800 |
|---|---|---|---|
| Ball Pressure Test | ISO 2309-1 | 115 N/mm | |
| Bending modulus | 2mm/mim | ISO 178 | 2200 Mpa |
| bending strength | 5mm/mim | ISO 178 | 95 Mpa |
| Elongation at Break | 50mm/mim | ISO 527-1-2 | >50 % |
| Tensile modulus | 1mm/mim | ISO 527-1-2 | 2300 Mpa |
| Tensile strain | 50mm/mim,Yield | ISO 527-1-2 | 7 % |
| Tensile stress | 50mm/mim,Yield | ISO 527-1-2 | 65 Mpa |
| Electrical performance | Test Condition | Test Method | COVESTRO GERMANY/1800 |
|---|---|---|---|
| Dissipation factor | 100Hz/1MHz | 1EC250 | 13/100 10 |
| Physical properties | Test Condition | Test Method | COVESTRO GERMANY/1800 |
|---|---|---|---|
| melt mass-flow rate | 330℃/2.16kg | ISO 1133 | 10/10 CM |
| 330℃/2.16kg | ISO 1133 | 10/10 g/(10min) | |
| Shrinkage rate | 垂直Flow | ISO 2577 | 0.85 % |
| Flow | ISO 2577 | 0.85 % | |
| Water absorption rate | 23℃Saturation值 | ISO 62 | 0.4 % |