Material Comparison
Add Comparison Model
Select Products for Comparison (1/4)
Highlight Differences
Hide Same
Product Name / Manufacturer / Model
Grade
Certificates
Reference Price
| mechanical properties | Test Condition | Test Method | JAPAN POLYPLASTIC/TR-10D |
|---|---|---|---|
| bending strength | ISO 178 | 90.0 Mpa | |
| Wear factor | 0.060MPa,0.15m/sec5 | JISK7218 | 600 10^-8mm³/N·m |
| Friction coefficient | Dynamic2 | JISK7218 | 0.34 |
| Wear factor | 0.060MPa,0.15m/sec7 | JISK7218 | 5000 10^-8mm³/N·m |
| Tensile strain | Break | ISO 527-2 | 5.0 % |
| Friction coefficient | Steel - Dynamic3 | JISK7218 | 0.44 |
| Bending modulus | ISO 178 | 3500 Mpa | |
| Tensile modulus | ISO 527-2 | 3700 Mpa | |
| tensile strength | ISO 527-2 | 57.0 Mpa | |
| Wear factor | 0.49MPa,0.30m/sec4 | JISK7218 | 10 10^-8mm³/N·m |
| 0.49MPa,0.30m/sec6 | JISK7218 | 2500 10^-8mm³/N·m | |
| impact performance | Test Condition | Test Method | JAPAN POLYPLASTIC/TR-10D |
| Charpy Notched Impact Strength | 23°C | ISO 179/1eA | 3.3 kJ/m² |
| Electrical performance | Test Condition | Test Method | JAPAN POLYPLASTIC/TR-10D |
| Volume resistivity | IEC 60093 | 3E+14 ohms·cm | |
| Surface resistivity | IEC 60093 | 2E+16 ohms | |
| Physical properties | Test Condition | Test Method | JAPAN POLYPLASTIC/TR-10D |
| Melt Volume Flow Rate (MVR) | 190°C/2.16kg | ISO 1133 | 31.0 cm3/10min |
| density | ISO 1183 | 1.48 g/cm³ | |
| Water absorption rate | 23°C,24hr | ISO 62 | 0.50 % |
| melt mass-flow rate | 190°C/2.16kg | ISO 1133 | 39 g/10min |
| flammability | Test Condition | Test Method | JAPAN POLYPLASTIC/TR-10D |
| UL flame retardant rating | UL 94 | HB | |
| Supplementary Information | Test Condition | Test Method | JAPAN POLYPLASTIC/TR-10D |
| ColourNumber | CF2001 | ||
| thermal performance | Test Condition | Test Method | JAPAN POLYPLASTIC/TR-10D |
| Linear coefficient of thermal expansion | MD:23to55°C | Internal Method | 9E-05 cm/cm/°C |
| TD:23to55°C | Internal Method | 9E-05 cm/cm/°C | |
| Hot deformation temperature | 1.8MPa,Unannealed | ISO 75-2/A | 112 °C |
| hardness | Test Condition | Test Method | JAPAN POLYPLASTIC/TR-10D |
| Rockwell hardness | M-Scale | ISO 2039-2 | 90 |