Material Comparison

Product Info
Product Name
Brand Name
Usages
Properties
Certificates
TPU C95A BASF JAPAN
Elastollan®
film、Food service sector、Automotive sector、Industrial machinery
high strength、High impact resistance、Aging resistance、High temperature resistan、Low temperature resistanc
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--

Plastic Datasheets

Mechanical propertiesTest ConditionTest MethodBASF JAPAN/C95A
Shore hardness邵氏 A,3 秒  Shore A, 3 secISO 761996
Wear amountIOS 113325 mm³
Shore hardness邵氏 D,3 秒  Shore D, 3 secISO 761947
Elastic bodyTest ConditionTest MethodBASF JAPAN/C95A
23℃,72 hr  23°C, 72 hrISO 81530 %
Tear strengthISO 34-1120 kN/m
70℃,24 hr  70°C, 24 hrISO 81545 %
Tensile strain断裂  BreakDIN 53504550 %
Tensile strength20% 应变  20% StrainDIN 535048 Mpa
屈服  YieldDIN 5350455 Mpa
屈服  DIN 5350440 Mpa
100% 应变  100%应变DIN 5350411 Mpa
Tensile strain断裂  Break   2 2DIN 53504500 %
Tensile strength300% 应变  300%应变DIN 5350422 Mpa
Flame retardant performanceTest ConditionTest MethodBASF JAPAN/C95A
UL flame retardant ratingUL 94HB
physical property Test ConditionTest MethodBASF JAPAN/C95A
DensityISO 1183/A1.21 g/cm³