PPS A410MX07 TORAY JAPAN
Torelina®
--
Filler: Glass mineral,70% filler by weight
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
Supplementary Information | Test Condition | Test Method | TORAY JAPAN/A410MX07 |
---|---|---|---|
BarFlowLength | 320°C,1.00mm | Internal Method | 7.50 CM |
hardness | Test Condition | Test Method | TORAY JAPAN/A410MX07 |
---|---|---|---|
Rockwell hardness | R-Sale | ISO 2039-2 | 123 |
thermal performance | Test Condition | Test Method | TORAY JAPAN/A410MX07 |
---|---|---|---|
Hot deformation temperature | 1.8MPa,Unannealed | ISO 75-2/A | 260 °C |
Linear coefficient of thermal expansion | TD | ISO 11359-2 | 2E-05 cm/cm/°C |
MD | ISO 11359-2 | 1.9E-05 cm/cm/°C | |
Melting temperature | ISO 11357-3 | 278 °C |
mechanical properties | Test Condition | Test Method | TORAY JAPAN/A410MX07 |
---|---|---|---|
Bending modulus | 23°C | ISO 178 | 25500 Mpa |
bending strength | 23°C | ISO 178 | 235 Mpa |
Tensile strain | Break,23°C | ISO 527-2 | 0.70 % |
tensile strength | 23°C | ISO 527-2 | 135 Mpa |
Electrical performance | Test Condition | Test Method | TORAY JAPAN/A410MX07 |
---|---|---|---|
Dielectric strength | IEC 60243-1 | 20 KV/mm | |
Volume resistivity | IEC 60093 | 1E+16 ohms·cm |
Physical properties | Test Condition | Test Method | TORAY JAPAN/A410MX07 |
---|---|---|---|
Shrinkage rate | TD:3.00mm2 | Internal Method | 0.45 % |
MD:3.00mm3 | Internal Method | 0.25 % | |
Water absorption rate | 23°C,24hr | ISO 62 | 0.020 % |
impact performance | Test Condition | Test Method | TORAY JAPAN/A410MX07 |
---|---|---|---|
Impact strength of simply supported beam without notch | 23°C | ISO 179 | 17 kJ/m² |
flammability | Test Condition | Test Method | TORAY JAPAN/A410MX07 |
---|---|---|---|
UL flame retardant rating | UL 94 | V-0 |