Material Comparison

Product Info
Product Name
Brand Name
Usages
Properties
Certificates
PES Paryls® PES F2250 Jiangmen Youju New Materials Co., Ltd.
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--

Plastic Datasheets

Impact resistanceTest ConditionTest MethodJiangmen Youju New Materials Co., Ltd./Paryls® PES F2250
Impact strength of cantilever beam gapISO 180/A6.5 kJ/m²
Electrical performanceTest ConditionTest MethodJiangmen Youju New Materials Co., Ltd./Paryls® PES F2250
Compared to the Leakage Tracking Index (CTI)IEC 60112PLC 4
dielectric constant100HzIEC 602503.90
dielectric strengthIEC 60243-137 kV/mm
Volume resistivityIEC 60093>1.0E+15 ohms·cm
Dissipation Factor100HzIEC 602501.7E-03
dielectric constant1MHzIEC 602503.80
Surface ResistivityIEC 60093>1.0E+15 ohms
Dissipation Factor1MHzIEC 602500.014
Mechanical propertiesTest ConditionTest MethodJiangmen Youju New Materials Co., Ltd./Paryls® PES F2250
tensile strength ISO 527-288.0 MPa
Tensile modulusISO 527-22700 MPa
Tensile strain屈服ISO 527-26.5 %
Flexural modulusISO 1782650 MPa
bending strengthISO 178120 MPa
flammabilityTest ConditionTest MethodJiangmen Youju New Materials Co., Ltd./Paryls® PES F2250
UL flame retardant rating1.5mmUL 94V-0
physical property Test ConditionTest MethodJiangmen Youju New Materials Co., Ltd./Paryls® PES F2250
melt mass-flow rate380°C/2.16kgISO 113318to28 g/10min
Shrinkage rateTDISO 294-40.86 %
MDISO 294-40.82 %
Water absorption rate平衡,23°C,50%RHISO 620.80 %
densityISO 11831.37 g/cm³
Thermal performanceTest ConditionTest MethodJiangmen Youju New Materials Co., Ltd./Paryls® PES F2250
Linear coefficient of thermal expansionMD:23°CISO 11359-25.2E-05 cm/cm/°C
Heat distortion temperature1.8MPa,未退火,HDTISO 75-2/A205 °C
Glass Transition TemperatureISO 11357-2225 °C

Contact Us

Get App

Top