Material Comparison
Product Info
Product Name
Brand Name
Usages
Properties
Certificates

LLDPE 6821WE SABIC SAUDI
SABIC®
chip、Food containers
High hardness
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
Other performance | Test Condition | Test Method | SABIC SAUDI/6821WE |
---|---|---|---|
Posterior adhesion | SABIC method | <10 g | |
Adhesive property | SABIC method | 10 g | |
antioxidant | SABIC method | + mg/kg | |
slip agent | SABIC method | 1500 mg/kg | |
antiblocking agent | SABIC method | 3500 mg/kg |
Basic performance | Test Condition | Test Method | SABIC SAUDI/6821WE |
---|---|---|---|
melt mass-flow rate | 190℃/2.16kg | ISO 1133 | 0.8 g/10min |
density | ISO 1183 | 921 kg/m3 |
Mechanical properties | Test Condition | Test Method | SABIC SAUDI/6821WE |
---|---|---|---|
yield stress | MD | ISO 527-3 | 12.5 Mpa |
elongation at break | MD | ISO 527-3 | 520 % |
ISO 8295 | 0.1 | ||
tear strength | TD | ISO 6383-2 | 350 kN/m |
MD | ISO 6383-2 | 70 kN/m | |
yield stress | TD | ISO 527-3 | 14 Mpa |
Elastic modulus | MD | ISO 527-3 | 220 Mpa |
Breaking stress | MD | ISO 527-3 | 35 Mpa |
TD | ISO 527-3 | 25 Mpa | |
elongation at break | TD | ISO 527-3 | 650 % |
Anti puncture ability | SABIC method | 450 J/m | |
Elastic modulus | TD | ISO 527-3 | 250 Mpa |
Impact Strength | ASTM D-4272 | 30 KJ/m |
optical performance | Test Condition | Test Method | SABIC SAUDI/6821WE |
---|---|---|---|
gloss | 45° | ASTM D-2457 | 45 ‰ |
transparency | SABIC method | 20 mV | |
Haze ratio | ASTM D-1003A | 20 % |
Thermal performance | Test Condition | Test Method | SABIC SAUDI/6821WE |
---|---|---|---|
vicat | 10N | ISO 306/B | 111 °C |
melting point | SABIC method | 125 °C |