| impact performance | Test Condition | Test Method | KAZANORGSINTEZ RUSSIA/010UL |
|---|---|---|---|
| Impact strength of cantilever beam gap | ASTM D256 | 68 kJ/m² | |
| Electrical performance | Test Condition | Test Method | KAZANORGSINTEZ RUSSIA/010UL |
| Dielectric loss | 0.009 | ||
| Dielectric strength | kV/mm | 20 | |
| Dielectric constant | 2.5 | ||
| mechanical properties | Test Condition | Test Method | KAZANORGSINTEZ RUSSIA/010UL |
| tensile strength | ASTM D 638 | 62 Mpa | |
| bending strength | ASTM D790 | 80 Mpa | |
| Tensile strain | ASTM D638 | 110 % | |
| Bending modulus | ASTM D790 | 2350 Mpa | |
| Physical properties | Test Condition | Test Method | KAZANORGSINTEZ RUSSIA/010UL |
| melt mass-flow rate | ASTM D1238 | 10±1.5 g/10min | |
| thermal performance | Test Condition | Test Method | KAZANORGSINTEZ RUSSIA/010UL |
| Vicat softening temperature | 150 °C |