Material Comparison
Product Info
Product Name
Brand Name
Usages
Properties
Certificates

POM MT8R02 CELANESE GERMANY
HOSTAFORM®
Fitness equipment,Automotive Applications,Thin walled products,Medical/nursing supplies
wear resistant,Good forming performance,Good liquidity,Good wear resistance
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
| thermal performance | Test Condition | Test Method | CELANESE GERMANY/MT8R02 |
|---|---|---|---|
| Hot deformation temperature | 1.8MPa,Unannealed | ISO 75-2/A | 82.0 °C |
| Melting temperature | ISO 11357-3 | 166 °C |
| mechanical properties | Test Condition | Test Method | CELANESE GERMANY/MT8R02 |
|---|---|---|---|
| Nominal tensile fracture strain | ISO 527-2/1A/50 | 30 % | |
| Tensile modulus | ISO 527-2/1A/1 | 2700 Mpa | |
| Tensile strain | Yield | ISO 527-2/1A/50 | 9.0 % |
| tensile strength | Yield | ISO 527-2/1A/50 | 62.0 Mpa |
| Physical properties | Test Condition | Test Method | CELANESE GERMANY/MT8R02 |
|---|---|---|---|
| density | ISO 1183 | 1.40 g/cm³ | |
| Melt Volume Flow Rate (MVR) | 190°C/2.16kg | ISO 1133 | 8.50 cm3/10min |
| impact performance | Test Condition | Test Method | CELANESE GERMANY/MT8R02 |
|---|---|---|---|
| Charpy Notched Impact Strength | 23°C | ISO 179/1eA | 8.0 kJ/m² |