Material Comparison
Product Info
Product Name
Brand Name
Usages
Properties
Certificates

ABS GF20 UMG JAPAN
UMG ABS®
Toy、Household daily necessiti、Automotive Applications、Electrical applications
Glass fiber reinforced
UL
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
hardness | Test Condition | Test Method | UMG JAPAN/GF20 |
---|---|---|---|
Rockwell hardness | R计秤,23°C | ISO 2039-2 | 117 |
Basic performance | Test Condition | Test Method | UMG JAPAN/GF20 |
---|---|---|---|
melt mass-flow rate | 8 g/10min |
Mechanical properties | Test Condition | Test Method | UMG JAPAN/GF20 |
---|---|---|---|
Charpy Notched Impact Strength | 7 kJ/m² | ||
Flexural modulus | ASTM D790/ISO 178 | 6.200 kg/cm²(MPa)[Lb/in²] | |
bending strength | 23°C | ISO 178 | 126 Mpa |
Flexural modulus | 6200 Mpa | ||
23°C | ISO 178 | 6200 Mpa | |
Tensile modulus | 23°C | ISO 527-2 | 7000 Mpa |
tensile strength | 断裂,23°C | ISO 527-2 | 96.0 Mpa |
Charpy Notched Impact Strength | ASTM D256/ISO 179 | 7 kg·cm/cm(J/M)ft·lb/in |
other | Test Condition | Test Method | UMG JAPAN/GF20 |
---|---|---|---|
characteristic | 玻纤 20% |
Physical properties | Test Condition | Test Method | UMG JAPAN/GF20 |
---|---|---|---|
melt mass-flow rate | ASTM D1238/ISO 1133 | 8 g/10min |
flammability | Test Condition | Test Method | UMG JAPAN/GF20 |
---|---|---|---|
UL flame retardant rating | 1.5mm | UL 94 | HB |
physical property | Test Condition | Test Method | UMG JAPAN/GF20 |
---|---|---|---|
Shrinkage rate | MD:23°C | ISO 294-4 | 0.10-0.40 % |
Melt volume flow rate | 220°C/10.0kg | ISO 1133 | 8.00 cm3/10min |
Thermal performance | Test Condition | Test Method | UMG JAPAN/GF20 |
---|---|---|---|
Heat distortion temperature | 1.8MPa,未退火,HDT | ISO 75-2/Af | 101 °C |
HDT | 101 °C | ||
Combustibility (rate) | UL 94 | HB | |
Heat distortion temperature | HDT | ASTM D648/ISO 75 | 101 ℃(℉) |
Linear coefficient of thermal expansion | MD | ISO 11359-2 | 4E-05 cm/cm/°C |
UL flame retardant rating | UL 94 | HB |