Material Comparison
Product Info
Product Name
Brand Name
Usages
Properties
Certificates

AES SE40 UMG JAPAN
DIALAC®
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
| hardness | Test Condition | Test Method | UMG JAPAN/SE40 |
|---|---|---|---|
| Rockwell hardness | R-Sale,23°C | ISO 2039-2 | 100 |
| Basic Performance | Test Condition | Test Method | UMG JAPAN/SE40 |
|---|---|---|---|
| melt mass-flow rate | 8 CM |
| thermal performance | Test Condition | Test Method | UMG JAPAN/SE40 |
|---|---|---|---|
| Hot deformation temperature | 1.8MPa,Unannealed | ISO 75-2/Af | 80.0 °C |
| HDT | 80 °C | ||
| Linear coefficient of thermal expansion | MD | ISO 11359-2 | 9E-05 cm/cm/°C |
| UL flame retardant rating | UL 94 | HB |
| mechanical properties | Test Condition | Test Method | UMG JAPAN/SE40 |
|---|---|---|---|
| Bending modulus | 2250 Mpa | ||
| 23°C | ISO 178 | 2250 Mpa | |
| bending strength | 23°C | ISO 178 | 69.0 Mpa |
| Charpy Notched Impact Strength | 27 KJ/m | ||
| Tensile modulus | 23°C | ISO 527-2 | 2200 Mpa |
| tensile strength | 23°C | ISO 527-2 | 45.0 Mpa |
| Physical properties | Test Condition | Test Method | UMG JAPAN/SE40 |
|---|---|---|---|
| Melt Volume Flow Rate (MVR) | 220°C/10.0kg | ISO 1133 | 8.00 cm3/10min |
| Shrinkage rate | MD:23°C | ISO 294-4 | 0.60-0.80 % |
| flammability | Test Condition | Test Method | UMG JAPAN/SE40 |
|---|---|---|---|
| UL flame retardant rating | 1.5mm | UL 94 | HB |