TPU 3491A COVESTRO GERMANY
Desmopan®
film,container,Thin walled products,Engineering accessories
High impact resistance,high strength
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
hardness | Test Condition | Test Method | COVESTRO GERMANY/3491A |
---|---|---|---|
Shore hardness | 邵氏 D, 15 sec | ISO 8683 | 40 |
邵氏 A, 3 sec | ISO 8683 | 92 | |
邵氏 A, 1 秒, 23°C | ISO 7619 | 92 | |
邵氏 D, 1 秒, 23°C | ISO 7619 | 40 |
Mechanical properties | Test Condition | Test Method | COVESTRO GERMANY/3491A |
---|---|---|---|
tensile strength | 10% 应变, 23°C | DIN 53504 | 3.90 Mpa |
Tensile storage modulus | 60°C | ISO 6721 | 59.0 Mpa |
wear resistance | ISO 4649 | 25.0 mm³ | |
tensile strength | 50% 应变, 23°C | DIN 53504 | 7.40 Mpa |
Tensile storage modulus | -20°C | ISO 6721 | 515 Mpa |
tensile strength | 断裂, 23°C | DIN 53504 | 54.1 Mpa |
300% 应变, 23°C | DIN 53504 | 25.8 Mpa | |
Tensile strain | 断裂, 23°C | DIN 53504 | 500 % |
Tensile storage modulus | 20°C | ISO 6721 | 94.0 Mpa |
tensile strength | 100% 应变, 23°C | DIN 53504 | 8.90 Mpa |
squeeze out | Test Condition | Test Method | COVESTRO GERMANY/3491A |
---|---|---|---|
drying temperature | < 80 °C | ||
Melt Temperature | 180 to 210 °C |
elastomer | Test Condition | Test Method | COVESTRO GERMANY/3491A |
---|---|---|---|
tear strength | 23°C | ISO 34-1 | 100 kN/m |
compression set | 70°C, 24 hr5 | ISO 815 | 50 % |
23°C, 72 hr | ISO 815 | 20 % | |
Resilience | ISO 4662 | 36 % |
injection | Test Condition | Test Method | COVESTRO GERMANY/3491A |
---|---|---|---|
Processing (melt) temperature | 190 to 210 °C | ||
drying temperature | < 80 °C | ||
Temperature | 20 to 40 °C |