Material Comparison

Product Info
Product Name
Brand Name
Usages
Properties
Certificates
PC IR2500 IDEMITSU JAPAN
TARFLON™ 
Automotive Applications,Home appliance components,Medical/nursing supplies,bottle
High mobility,Medium viscosity
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--

Plastic Datasheets

Impact resistanceTest ConditionTest MethodIDEMITSU JAPAN/IR2500
Impact strength of cantilever beam gap3.20mmASTM D256830 J/m
hardnessTest ConditionTest MethodIDEMITSU JAPAN/IR2500
Rockwell hardnessM级ASTM D78575
R级ASTM D785120
Electrical performanceTest ConditionTest MethodIDEMITSU JAPAN/IR2500
Dissipation Factor60HzASTM D1506.6E-04
dielectric constant60HzASTM D1502.91
Volume resistivityASTM D2571E+16 ohms·cm
Dissipation Factor1MHzASTM D1509.2E-03
dielectric constant1MHzASTM D1502.85
dielectric strength1.60mmASTM D14929 KV/mm
arc resistanceASTM D495110 sec
Mechanical propertiesTest ConditionTest MethodIDEMITSU JAPAN/IR2500
elongation断裂ASTMD638110 %
Flexural modulusASTMD7902350 Mpa
tensile strength 屈服ASTMD63873.0 Mpa
断裂ASTMD63878.0 Mpa
Tensile modulusASTMD6382300 Mpa
bending strengthASTMD79095.0 Mpa
optical performance Test ConditionTest MethodIDEMITSU JAPAN/IR2500
refractive indexASTMD5421.586
transmissivityASTM D100389.0 %
flammabilityTest ConditionTest MethodIDEMITSU JAPAN/IR2500
UL flame retardant rating3.0mmUL 94HB
Hot filament ignition temperature3.2mmIEC 60695-2-13960 °C
physical property Test ConditionTest MethodIDEMITSU JAPAN/IR2500
Shrinkage rateMDASTM D9550.50-0.70 %
densityASTMD7921.20 g/cm³
melt mass-flow rate300°C/1.2kgASTMD12388.0 g/10min
Water absorption rate23°C,24hrASTM D5700.23 %
Thermal performanceTest ConditionTest MethodIDEMITSU JAPAN/IR2500
Heat distortion temperature1.8MPa,未退火,HDTASTMD648135 °C
Linear coefficient of thermal expansionMDASTM D6966.5E-05 cm/cm/°C

Contact Us