Material Comparison
Product Info
Product Name
Brand Name
Usages
Properties
Certificates

PA66 CM3003G-30BK TORAY JAPAN
Amilan®
Electrical components,OA device
Flame retardant,Glass fiber reinforced
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
| machinability | Test Condition | Test Method | TORAY JAPAN/CM3003G-30BK |
|---|---|---|---|
| Shrinkage rate | 1mmt | 0.2-0.4 % | |
| 3mmt | 0.6-0.8 % |
| thermal performance | Test Condition | Test Method | TORAY JAPAN/CM3003G-30BK |
|---|---|---|---|
| Hot deformation temperature | 1.86MPa | D648 | 255 °C |
| 0.46Mpa | D648 | 262 °C | |
| Melting temperature | DSC | 265 °C | |
| UL flame retardant rating | UL 94 | HB |
| mechanical properties | Test Condition | Test Method | TORAY JAPAN/CM3003G-30BK |
|---|---|---|---|
| Bending modulus | 23℃ | D790 | 10.0 GPa |
| bending strength | 23℃ | D790 | 270 Mpa |
| Elongation at Break | 23℃ | D638 | 5 % |
| Impact strength of cantilever beam gap | 23℃ | D256 | 85 J/m |
| tensile strength | Yield,23℃ | D638 | 170 Mpa |
| Wear resistance | D1044 | 23 mg/1000 |
| Physical properties | Test Condition | Test Method | TORAY JAPAN/CM3003G-30BK |
|---|---|---|---|
| density | D792 | 1.38 | |
| Rockwell hardness | 23℃ | D785 | 121 R |
| Water absorption rate | 23℃,24hrs | D570 | 0.6 % |
| 23℃,水中 | D570 | 5.5 % |