Material Comparison
Product Info
Product Name
Brand Name
Usages
Properties
Certificates

PUR,Unspecified EN-21 ELANTAS PDG Inc.
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
| hardness | Test Condition | Test Method | ELANTAS PDG Inc./EN-21 |
|---|---|---|---|
| Shore hardness | ShoreA | 80 |
| Supplementary Information | Test Condition | Test Method | ELANTAS PDG Inc./EN-21 |
|---|---|---|---|
| PeakExotherm | 69 °C |
| thermal performance | Test Condition | Test Method | ELANTAS PDG Inc./EN-21 |
|---|---|---|---|
| Linear coefficient of thermal expansion | MD | 3.8E-04 cm/cm/°C | |
| thermal conductivity | 0.30 W/m/K |
| Electrical performance | Test Condition | Test Method | ELANTAS PDG Inc./EN-21 |
|---|---|---|---|
| Dielectric constant | 1kHz | 3.40 | |
| Dielectric strength | 1.59mm | 26 kV/mm | |
| Dissipation factor | 1kHz | 0.017 | |
| insulation resistance | >2.5E+13 ohms | ||
| Surface resistivity | >1.0E+15 ohms | ||
| Volume resistivity | 7.2E+14 ohms·cm |
| thermosetting | Test Condition | Test Method | ELANTAS PDG Inc./EN-21 |
|---|---|---|---|
| GelTime | 60°C | 0.3 hr | |
| 25°C7 | 1.5 hr | ||
| storage stability | 25°C7 | 40 min | |
| 60°C | 8.0 min | ||
| stripping time | 25°C | 10000 min | |
| 80°C | 240 min | ||
| Thermosetting components | 按重量计算的混合比 | 100 | |
| Hardener | 按重量计算的混合比:120 | ||
| Thermosetting mixed viscosity | 60°C | 320 cP | |
| 25°C | 2000 cP |
| Physical properties | Test Condition | Test Method | ELANTAS PDG Inc./EN-21 |
|---|---|---|---|
| density | --4 | 1.07 g/cm³ | |
| --5 | 1.14 g/cm³ | ||
| 吸水率(25°C,24hr) | 0.070 % | ||
| --3 | 0.958 g/cm³ | ||
| viscosity | Resin:25°C | 6000 mPa·s | |
| Hardener:25°C | 800 mPa·s |
| Cured Properties | Test Condition | Test Method | ELANTAS PDG Inc./EN-21 |
|---|---|---|---|
| Shrinkage rate | 1.4 % |
| flammability | Test Condition | Test Method | ELANTAS PDG Inc./EN-21 |
|---|---|---|---|
| UL flame retardant rating | UL 94 | HB |
| elastomer | Test Condition | Test Method | ELANTAS PDG Inc./EN-21 |
|---|---|---|---|
| elongation | Break | 160 % | |
| Permanent compression deformation | 10 % | ||
| tear strength | 20.8 kN/m | ||
| tensile strength | Yield | 13.8 MPa |