| film | Test Condition | Test Method | STYRON US/1430 |
|---|---|---|---|
| Elmendorf tear strength | TD:51μm | ASTM D1922 | 730 g |
| MD:51μm | ASTM D1922 | 470 g | |
| tensile strength | MD:Break,51μm | ASTMD882 | 30.6 Mpa |
| TD:Yield,51μm | ISO 527-3 | 10.2 Mpa | |
| TD:Yield,51μm | ASTM D882 | 10.2 Mpa | |
| TD:Break,51μm | ASTMD882 | 31.0 Mpa | |
| Elmendorf tear strength | MD:51μm | ISO 6383-2 | 2100 N |
| elongation | TD:Break,51μm | ASTMD882 | 470 % |
| tensile strength | MD:Yield,51μm | ASTM D882 | 10.4 Mpa |
| elongation | MD:Break,51μm | ASTMD882 | 420 % |
| tensile strength | MD:Yield,51μm | ISO 527-3 | 10.4 Mpa |
| Elmendorf tear strength | TD:51μm | ISO 6383-2 | 3300 N |
| Physical properties | Test Condition | Test Method | STYRON US/1430 |
| Content of comonomer | Internal Method | 9.7 % | |
| density | ISO 1183 | 0.93 g/cm³ | |
| ASTM D-792 | 0.93 g/cm³ | ||
| ASTMD792 | 0.930 g/cm³ | ||
| melt mass-flow rate | 190°C/2.16kg | ASTMD1238 | 5.0 g/10min |
| optical performance | Test Condition | Test Method | STYRON US/1430 |
| turbidity | 50.8μm | ASTM D1003 | 4.0 % |
| 50.8μm | ISO 14782 | 4.0 % | |
| gloss | 45°,50.8μm | ASTM D2457 | 74 |
| 45°,50.8um | ASTM D-2457 | 74 | |
| turbidity | 50.8um | ASTM D-1003 | 4 % |
| 50.8um | ISO 14782 | 4 % | |
| mechanical properties | Test Condition | Test Method | STYRON US/1430 |
| tensile strength | Yield,Compression Molded | ASTM D-638 | 7.67 MPa |
| 50.8um,Yield,TD | ISO 527-3 | 10.2 MPa | |
| Break,Compression Molded4 | ASTM D638 | 19.5 Mpa | |
| Break,Compression Molded | ISO 527-2/508 | 19.5 Mpa | |
| Compression Molded,Break | ISO 527-2/508 | 19.5 MPa | |
| 50.8um,MD,Break | ASTM D-882 | 30.6 MPa | |
| Elongation at Break | 50.8um,MD | ASTM D-882 | 420 % |
| tensile strength | 50.8um,MD,Break | ISO 527-3 | 30.6 MPa |
| Elongation at Break | 50.8um,TD | ASTM D-882 | 470 % |
| Elmendorf tear strength | 50.8um,MD | ASTM D-1922 | 470 g |
| tensile strength | 50.8um,Yield,MD | ISO 527-3 | 10.4 MPa |
| Elongation at Break | Compression Molded | ISO 527-2/508 | 580 % |
| Compression Molded | ASTM D-638 | 580 % | |
| Elmendorf tear strength | 50.8um,TD | ISO 6383-2 | 3300 N |
| tensile strength | Yield,Compression Molded4 | ASTM D638 | 7.67 Mpa |
| 50.8um,Yield,TD | ASTM D-882 | 10.2 MPa | |
| Elmendorf tear strength | 50.8um,TD | ASTM D-1922 | 730 g |
| 50.8um,MD | ISO 6383-2 | 2100 N | |
| Elongation at Break | 50.8um,TD | ISO 527-3 | 470 % |
| tensile strength | 50.8um,Yield,MD | ASTM D-882 | 10.4 MPa |
| 50.8um,TD,Break | ASTM D-882 | 31.0 MPa | |
| Yield,Compression Molded | ISO 527-2/508 | 7.67 MPa | |
| Compression Molded,Break | ASTM D-638 | 19.5 MPa | |
| elongation | Break,Compression Molded | ISO 527-2/508 | 580 % |
| Break,Compression Molded4 | ASTM D638 | 580 % | |
| tensile strength | 50.8um,TD,Break | ISO 527-3 | 31 MPa |
| Elongation at Break | 50.8um,MD | ISO 527-3 | 420 % |
| thermal performance | Test Condition | Test Method | STYRON US/1430 |
| Vicat softening temperature | ASTMD1525 | 76.1 °C | |
| Melting temperature | Internal Method | 96.1 ℃ | |
| Vicat softening temperature | ISO 306 | 76.1 ℃ | |
| ASTM D-1525 | 76.1 ℃ | ||
| Basic Performance | Test Condition | Test Method | STYRON US/1430 |
| melt mass-flow rate | 190℃/2.16kg | ASTM D-1238 | 5 g/10min |
| Monomer content | Internal Method | 9.7 % | |
| melt mass-flow rate | 190℃/2.16kg | ISO 1133 | 5 g/10min |